MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.

Data provided by the manufacturer.

Solvay Specialty Polymers has acquired the Ryton product line. This product was discontinued prior to the acquisition and is listed under the Chevron Phillips name for historical purposes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 g/ccASTM D792
Water Absorption 0.070 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118
Tensile Strength, Ultimate 97.0 MPaASTM D638
Tensile Strength, Yield 97.0 MPaASTM D638
Elongation at Break 0.70 %ASTM D638
Flexural Yield Strength 131 MPaASTM D790
Flexural Modulus 17.0 GPaASTM D790
Compressive Yield Strength 120 MPaASTM D695
Shear Strength 70.0 MPaEstimated from similar grades.; ASTM D732
Izod Impact, Notched 0.370 J/cmASTM D256
Izod Impact, Unnotched 1.10 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 6.00e+15 ohm-cmASTM D257
Surface Resistance 5.00e+8 ohm
@Temperature 90.0 °C
95% RH, 48 hrs
Dielectric Constant 4.5
@Frequency 1e+6 Hz
ASTM D150
 4.7
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 12.8 kV/mmASTM D149
Dissipation Factor 0.0070
@Frequency 1e+6 Hz
ASTM D150
 0.0090
@Frequency 1000 Hz
ASTM D150
Arc Resistance 182 secASTM D495
Comparative Tracking Index 240 VUL 746A
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.190 BTU/lb-°F
 0.770 J/g-°C
Thermal Conductivity 0.600 W/m-K
Melting Point 285 °C
Maximum Service Temperature, Air 220 - 240 °CUL temperature Index
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °CASTM D648
Glass Transition Temp, Tg 88.0 °C
Flammability, UL94 5VAV-0/5VA UL-94 Rating
Oxygen Index 53 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 304 - 343 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS); Molded
Chevron Phillips Ryton® R10-110BL Polyphenylene Sulfide Compound
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
Overview of materials for Polyphenylene Sulfide (PPS) Coating Resin

PZPSR51 / 58229

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.