MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Overview of materials for Polyphenylene Sulfide (PPS); Molded
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS); Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.18 - 2.26 g/cc0.0426 - 0.0816 lb/in³Average value: 1.59 g/cc Grade Count:34
Water Absorption 0.0100 - 0.0500 %0.0100 - 0.0500 %Average value: 0.0327 % Grade Count:11
Water Absorption at Saturation 0.0200 - 0.100 %0.0200 - 0.100 %Average value: 0.0700 % Grade Count:5
Viscosity  180000 - 240000 cP
@Temperature 310 - 310 °C
180000 - 240000 cP
@Temperature 590 - 590 °F
Average value: 220000 cP Grade Count:3
 180000 - 240000 cP
@Frequency 100 - 100 Hz
180000 - 240000 cP
@Frequency 100 - 100 Hz
Average value: 220000 cP Grade Count:3
Maximum Moisture Content 0.02000.0200Average value: 0.0200 Grade Count:6
Linear Mold Shrinkage 0.00200 - 0.0200 cm/cm0.00200 - 0.0200 in/inAverage value: 0.00924 cm/cm Grade Count:23
Linear Mold Shrinkage, Transverse 0.00300 - 0.0210 cm/cm0.00300 - 0.0210 in/inAverage value: 0.00956 cm/cm Grade Count:17
Melt Flow 27.0 - 2000 g/10 min27.0 - 2000 g/10 minAverage value: 398 g/10 min Grade Count:13
Ash 0.400 - 0.800 %0.400 - 0.800 %Average value: 0.600 % Grade Count:10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 90.0 - 10490.0 - 104Average value: 97.1 Grade Count:7
Tensile Strength, Ultimate 27.6 - 155 MPa4000 - 22500 psiAverage value: 82.4 MPa Grade Count:26
 59.0191 - 59.0191 MPa
@Temperature -40.0 - -40.0 °C
8560.01 - 8560.01 psi
@Temperature -40.0 - -40.0 °F
Average value: 59.0 MPa Grade Count:1
Tensile Strength, Yield 46.0 - 104 MPa6670 - 15100 psiAverage value: 64.4 MPa Grade Count:8
 79.9792 - 79.9792 MPa
@Temperature -40.0 - -40.0 °C
11600.0 - 11600.0 psi
@Temperature -40.0 - -40.0 °F
Average value: 80.0 MPa Grade Count:1
Elongation at Break 0.350 - 80.0 %0.350 - 80.0 %Average value: 25.1 % Grade Count:23
Modulus of Elasticity 1.65 - 17.2 GPa239 - 2500 ksiAverage value: 6.31 GPa Grade Count:15
 2.86132 - 2.86132 GPa
@Temperature -40.0 - -40.0 °C
415.006 - 415.006 ksi
@Temperature -40.0 - -40.0 °F
Average value: 2.86 GPa Grade Count:1
Flexural Yield Strength 50.0 - 703 MPa7250 - 102000 psiAverage value: 158 MPa Grade Count:33
Flexural Modulus 1.50 - 21.0 GPa218 - 3050 ksiAverage value: 9.37 GPa Grade Count:33
Poissons Ratio 0.370 - 0.4100.370 - 0.410Average value: 0.392 Grade Count:4
Izod Impact, Notched 0.310 - 0.801 J/cm0.580 - 1.50 ft-lb/inAverage value: 0.555 J/cm Grade Count:9
Izod Impact, Unnotched 0.534 - 13.0 J/cm1.00 - 24.4 ft-lb/inAverage value: 5.23 J/cm Grade Count:6
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²
@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 7.00 kJ/m² Grade Count:1
Charpy Impact Unnotched 1.30 - 2100 J/cm²6.20 - 9990 ft-lb/in²Average value: 2.56 J/cm² Grade Count:8
 2.80 - 2.80 J/cm²
@Temperature -30.0 - -30.0 °C
13.3 - 13.3 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 2.80 J/cm² Grade Count:1
Charpy Impact, Notched 0.250 - 6.93 J/cm²1.19 - 33.0 ft-lb/in²Average value: 2.60 J/cm² Grade Count:17
 0.700 - 5.04 J/cm²
@Temperature -30.0 - -30.0 °C
3.33 - 24.0 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 2.58 J/cm² Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 - 1.00e+17 ohm-cm1.00e+14 - 1.00e+17 ohm-cmAverage value: 3.02e+16 ohm-cm Grade Count:13
Surface Resistance 1e+05 - 1.00e+15 ohm1e+05 - 1.00e+15 ohmAverage value: 5.50e+14 ohm Grade Count:3
 1.00e+12 - 1.00e+12 ohm
@Temperature 90.0 - 90.0 °C
1.00e+12 - 1.00e+12 ohm
@Temperature 194 - 194 °F
Average value: 1.00e+12 ohm Grade Count:2
Dielectric Constant 3.00 - 12.03.00 - 12.0Average value: 4.49 Grade Count:20
Dielectric Strength 9.00 - 30.0 kV/mm229 - 762 kV/inAverage value: 21.1 kV/mm Grade Count:14
Dissipation Factor 0.000300 - 0.1000.000300 - 0.100Average value: 0.00758 Grade Count:20
Arc Resistance 20.0 - 126 sec20.0 - 126 secAverage value: 81.3 sec Grade Count:6
Comparative Tracking Index 150 - 200 V150 - 200 VAverage value: 168 V Grade Count:7
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 - 97.2 µm/m-°C5.56 - 54.0 µin/in-°FAverage value: 35.3 µm/m-°C Grade Count:24
 59.94 - 140 µm/m-°C
@Temperature 22.8 - 200 °C
33.30 - 77.8 µin/in-°F
@Temperature 73.0 - 392 °F
Average value: 112 µm/m-°C Grade Count:6
CTE, linear, Transverse to Flow 17.0 - 122 µm/m-°C9.44 - 68.0 µin/in-°FAverage value: 46.8 µm/m-°C Grade Count:19
 97.2 - 140.4 µm/m-°C
@Temperature 70.0 - 200 °C
54.0 - 78.00 µin/in-°F
@Temperature 158 - 392 °F
Average value: 128 µm/m-°C Grade Count:5
Specific Heat Capacity 1.00 - 1.67 J/g-°C0.239 - 0.399 BTU/lb-°FAverage value: 1.39 J/g-°C Grade Count:3
Thermal Conductivity 0.251 - 13.3 W/m-K1.74 - 92.0 BTU-in/hr-ft²-°FAverage value: 2.64 W/m-K Grade Count:8
Melting Point 280 - 284 °C536 - 543 °FAverage value: 281 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 149 - 281 °C300 - 538 °FAverage value: 248 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 75.0 - 270 °C167 - 518 °FAverage value: 181 °C Grade Count:27
Vicat Softening Point 120 - 270 °C248 - 518 °FAverage value: 188 °C Grade Count:3
Flammability, UL94 HB - V-0HB - V-0Grade Count:26
Oxygen Index 44.0 - 49.0 %44.0 - 49.0 %Average value: 46.7 % Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 340 °C68.0 - 644 °FAverage value: 188 °C Grade Count:13
Nozzle Temperature 290 - 338 °C554 - 640 °FAverage value: 314 °C Grade Count:9
Adapter Temperature 290 - 310 °C554 - 590 °FAverage value: 300 °C Grade Count:3
Die Temperature 300 - 320 °C572 - 608 °FAverage value: 310 °C Grade Count:3
Melt Temperature 270 - 345 °C518 - 653 °FAverage value: 310 °C Grade Count:13
Mold Temperature 50.0 - 180 °C122 - 356 °FAverage value: 135 °C Grade Count:14
Drying Temperature 80.0 - 150 °C176 - 302 °FAverage value: 106 °C Grade Count:13
Injection Pressure 34.5 - 103 MPa5000 - 15000 psiAverage value: 80.4 MPa Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

O4500 / 78334

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.