MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.

Data provided by the manufacturer.

Solvay Specialty Polymers has acquired the Ryton product line. This product was discontinued prior to the acquisition and is listed under the Chevron Phillips name for historical purposes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc0.0596 lb/in³ASTM D792
Water Absorption 0.050 %0.050 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 123123
Tensile Strength, Ultimate 145 MPa21000 psiASTM D638
Tensile Strength, Yield 145 MPa21000 psiASTM D638
Elongation at Break 1.1 %1.1 %ASTM D638
Modulus of Elasticity 15.0 GPa2180 ksiASTM D638
Flexural Yield Strength 186 MPa27000 psiASTM D790
Flexural Modulus 14.0 GPa2030 ksiASTM D790
Compressive Yield Strength 179 MPa26000 psiASTM D695
Poissons Ratio 0.3840.384
Fatigue Strength 58.0 MPa
@# of Cycles 1.00e+6
8410 psi
@# of Cycles 1.00e+6
10 Hz, ASTM Type I tensile bar
Shear Modulus 5.42 GPa786 ksiCalculated
Shear Strength 90.0 MPa13100 psiASTM D732
Izod Impact, Notched 0.740 J/cm1.39 ft-lb/inASTM D256
Izod Impact, Unnotched 3.20 J/cm5.99 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 4.50e+16 ohm-cm4.50e+16 ohm-cmASTM D257
Surface Resistance 1.00e+13 ohm
@Temperature 90.0 °C
1.00e+13 ohm
@Temperature 194 °F
95% RH, 48 hrs
Insulation Resistance 1.00e+11 ohm1.00e+11 ohmAccelerated; 194°F; 95% RH; 2 days; ASTM D257
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
ASTM D150
 4.1
@Frequency 1000 Hz
4.1
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 14.0 kV/mm356 kV/inASTM D149
Dissipation Factor  0.0022
@Frequency 1000 Hz
0.0022
@Frequency 1000 Hz
ASTM D150
 0.0036
@Frequency 1e+6 Hz
0.0036
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 124 sec124 secASTM D495
Comparative Tracking Index 160 V160 VUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.0 µm/m-°C
@Temperature 100 °C
6.67 µin/in-°F
@Temperature 212 °F
 18.0 µm/m-°C
@Temperature -100 °C
10.0 µin/in-°F
@Temperature -148 °F
 40.0 µm/m-°C
@Temperature 20.0 °C
22.2 µin/in-°F
@Temperature 68.0 °F
In machine direction.
 100 µm/m-°C
@Temperature 250 °C
55.6 µin/in-°F
@Temperature 482 °F
CTE, linear, Transverse to Flow  22.0 µm/m-°C
@Temperature 250 °C
12.2 µin/in-°F
@Temperature 482 °F
 30.0 µm/m-°C
@Temperature -100 °C
16.7 µin/in-°F
@Temperature -148 °F
 40.0 µm/m-°C
@Temperature 20.0 °C
22.2 µin/in-°F
@Temperature 68.0 °F
 80.0 µm/m-°C
@Temperature 100 °C
44.4 µin/in-°F
@Temperature 212 °F
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°FEstimated from similar grades.
Thermal Conductivity 0.290 W/m-K2.01 BTU-in/hr-ft²-°FEstimated from similar grades.
Melting Point 285 °C545 °F
Maximum Service Temperature, Air 200 - 220 °C392 - 428 °FUL temperature Index
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FASTM D648
Glass Transition Temp, Tg 88.0 °C190 °F
Flammability, UL94 5VA5VAV-0/5VA UL-94 Rating
Oxygen Index 50 %50 %Estimated from similar grades.; ASTM D2863
 
Processing PropertiesMetricEnglishComments
Melt Temperature 304 - 343 °C579 - 649 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
Overview of materials for Nylon 66, 50% Glass Fiber Filled
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)
Delrin Delrin® 150 NC010 POM

PZPSR42 / 58222

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.