MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.

Data provided by the manufacturer.

Solvay Specialty Polymers has acquired the Ryton product line. This product was discontinued prior to the acquisition and is listed under the Chevron Phillips name for historical purposes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120
Tensile Strength, Ultimate 120 MPa17400 psiASTM D638
Tensile Strength, Yield 120 MPa17400 psiASTM D638
Elongation at Break 1.0 %1.0 %ASTM D638
Modulus of Elasticity 13.0 GPa1890 ksiASTM D638
Flexural Yield Strength 170 MPa24700 psiASTM D790
Flexural Modulus 12.0 GPa1740 ksiASTM D790
Compressive Yield Strength 170 MPa24700 psiASTM D695
Poissons Ratio 0.3960.396
Shear Modulus 4.66 GPa676 ksiCalculated
Shear Strength 82.7 MPa12000 psi
Izod Impact, Notched 0.530 J/cm0.993 ft-lb/inASTM D256
Izod Impact, Unnotched 2.40 J/cm4.50 ft-lb/inASTM D256
Taber Abrasion, mg/1000 Cycles 2323CS-17 wheel; 1 kg
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.40e+15 ohm-cm1.40e+15 ohm-cmASTM D257
Insulation Resistance 1.00e+11 ohm1.00e+11 ohmAccelerated; 194°F; 95% RH; 2 days; ASTM D257
Dielectric Strength 19.1 kV/mm485 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear  18.0 µm/m-°C
@Temperature -100 °C
10.0 µin/in-°F
@Temperature -148 °F
 20.0 µm/m-°C
@Temperature 250 °C
11.1 µin/in-°F
@Temperature 482 °F
 35.0 µm/m-°C
@Temperature 20.0 °C
19.4 µin/in-°F
@Temperature 68.0 °F
In machine direction.
CTE, linear, Transverse to Flow  25.0 µm/m-°C
@Temperature -100 °C
13.9 µin/in-°F
@Temperature -148 °F
 35.0 µm/m-°C
@Temperature 20.0 °C
19.4 µin/in-°F
@Temperature 68.0 °F
 60.0 µm/m-°C
@Temperature 250 °C
33.3 µin/in-°F
@Temperature 482 °F
Thermal Conductivity 0.320 W/m-K
@Temperature 90.0 °C
2.22 BTU-in/hr-ft²-°F
@Temperature 194 °F
Melting Point 285 °C545 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FEstimated from similar grades. ASTM D648
Glass Transition Temp, Tg 88.0 °C190 °F
Flammability, UL94 5VA5VAV-0/5VA UL-94 Rating (value for most Ryton® grades)
Oxygen Index 50 %50 %Estimated from similar grades.; ASTM D2863
 
Processing PropertiesMetricEnglishComments
Melt Temperature 304 - 343 °C579 - 649 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
Celanese FORTRON 214 PPS, Unfilled
Chevron Phillips Ryton® BR42C Polyphenylene Sulfide Compound
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)

PZPSR44 / 58224

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.