MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.

Data provided by the manufacturer.

Solvay Specialty Polymers has acquired the Ryton product line. This product was discontinued prior to the acquisition and is listed under the Chevron Phillips name for historical purposes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120
Tensile Strength, Ultimate 120 MPaASTM D638
Tensile Strength, Yield 120 MPaASTM D638
Elongation at Break 1.0 %ASTM D638
Modulus of Elasticity 13.0 GPaASTM D638
Flexural Yield Strength 170 MPaASTM D790
Flexural Modulus 12.0 GPaASTM D790
Compressive Yield Strength 170 MPaASTM D695
Poissons Ratio 0.396
Shear Modulus 4.66 GPaCalculated
Shear Strength 12000 psi
Izod Impact, Notched 0.530 J/cmASTM D256
Izod Impact, Unnotched 2.40 J/cmASTM D256
Taber Abrasion, mg/1000 Cycles 23CS-17 wheel; 1 kg
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.40e+15 ohm-cmASTM D257
Insulation Resistance 1.00e+11 ohmAccelerated; 194°F; 95% RH; 2 days; ASTM D257
Dielectric Strength 19.1 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature -100 °C
 20.0 µm/m-°C
@Temperature 250 °C
 35.0 µm/m-°C
@Temperature 20.0 °C
In machine direction.
CTE, linear, Transverse to Flow 25.0 µm/m-°C
@Temperature -100 °C
 35.0 µm/m-°C
@Temperature 20.0 °C
 60.0 µm/m-°C
@Temperature 250 °C
Thermal Conductivity 0.320 W/m-K
@Temperature 90.0 °C
Melting Point 285 °C
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °CEstimated from similar grades. ASTM D648
Glass Transition Temp, Tg 88.0 °C
Flammability, UL94 5VAV-0/5VA UL-94 Rating (value for most Ryton® grades)
Oxygen Index 50 %Estimated from similar grades.; ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 304 - 343 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
Celanese FORTRON 214 PPS, Unfilled
Chevron Phillips Ryton® BR42C Polyphenylene Sulfide Compound
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)

PZPSR44 / 58224

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.