MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Natural Color Polyphenylene Sulfide Compound

Ryton® R-7 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compound with the inherent cost savings of thermoplastics.

Applications: Switches

Comments: Test specimen molding conditions: Stock Temperature, 315-345°C; Mold Temperature, 135°C; ASTM Values Converted to SI Units

Data provided by Chevron Phillips Chemical Company LP.

Solvay Specialty Polymers has acquired the Ryton product line. This product was discontinued prior to the acquisition and is listed under the Chevron Phillips name for historical purposes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³ASTM D792
Water Absorption 0.030 %0.030 %ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/in102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inMeasured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 135 MPa19600 psiASTM D638
Elongation at Break 0.90 %0.90 %ASTM D638
Modulus of Elasticity 17.2 GPa2500 ksi
Flexural Yield Strength 215 MPa31200 psiASTM D790
Flexural Modulus 18.0 GPa2610 ksiASTM D790
Compressive Yield Strength 240 MPa34800 psiASTM D695
Poissons Ratio 0.3570.357
Shear Modulus 6.34 GPa920 ksiCalculated
Izod Impact, Notched 0.750 J/cm1.41 ft-lb/inASTM D256
Izod Impact, Unnotched 2.90 J/cm5.43 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 5.00e+15 ohm-cm5.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+12 ohm
@Temperature 90.0 °C
1.00e+12 ohm
@Temperature 194 °F
95% RH, 48 hrs
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
ASTM D150
 5.1
@Frequency 1000 Hz
5.1
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm457 kV/inASTM D149
Dissipation Factor  0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
ASTM D150
 0.060
@Frequency 1000 Hz
0.060
@Frequency 1000 Hz
ASTM D150
Arc Resistance 150 sec150 secASTM D495
Comparative Tracking Index 225 V225 VUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 100 - 200 °C
6.11 µin/in-°F
@Temperature 212 - 392 °F
Axial; ASTM E831
 17.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
9.44 µin/in-°F
@Temperature -58.0 - 122 °F
Axial; ASTM E831
CTE, linear, Transverse to Flow  31.0 µm/m-°C
@Temperature 20.0 °C
17.2 µin/in-°F
@Temperature 68.0 °F
ASTM E831
 70.0 µm/m-°C
@Temperature 100 - 200 °C
38.9 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
Thermal Conductivity 0.600 W/m-K4.16 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °FUL Temperature Index 200 / 220 per UL746B
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FAnnealed 2 hr @ 200°C; ASTM D665
Flammability, UL94 5VA5VAUL94 V-0/5VA

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
Mitsubishi Chemical Advanced Materials Semitron™ ESd 420 PEI Static Dissipative Polyetherimide
Mitsubishi Chemical Advanced Materials Semitron™ ESd 420 V PEI
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin

PZCHEVY34 / 20603

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.