MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.

Data provided by the manufacturer.

Solvay Specialty Polymers has acquired the Ryton product line. This product was discontinued prior to the acquisition and is listed under the Chevron Phillips name for historical purposes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³ASTM D792
Water Absorption 0.070 %0.070 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118
Tensile Strength, Ultimate 97.0 MPa14100 psiASTM D638
Tensile Strength, Yield 97.0 MPa14100 psiASTM D638
Elongation at Break 0.70 %0.70 %ASTM D638
Flexural Yield Strength 131 MPa19000 psiASTM D790
Flexural Modulus 17.0 GPa2470 ksiASTM D790
Compressive Yield Strength 120 MPa17400 psiASTM D695
Shear Strength 70.0 MPa10200 psiEstimated from similar grades.; ASTM D732
Izod Impact, Notched 0.370 J/cm0.693 ft-lb/inASTM D256
Izod Impact, Unnotched 1.10 J/cm2.06 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 6.00e+15 ohm-cm6.00e+15 ohm-cmASTM D257
Surface Resistance 5.00e+8 ohm
@Temperature 90.0 °C
5.00e+8 ohm
@Temperature 194 °F
95% RH, 48 hrs
Dielectric Constant  4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
ASTM D150
 4.7
@Frequency 1000 Hz
4.7
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 12.8 kV/mm325 kV/inASTM D149
Dissipation Factor  0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
ASTM D150
 0.0090
@Frequency 1000 Hz
0.0090
@Frequency 1000 Hz
ASTM D150
Arc Resistance 182 sec182 secASTM D495
Comparative Tracking Index 240 V240 VUL 746A
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.770 J/g-°C0.184 BTU/lb-°F
 0.795 J/g-°C0.190 BTU/lb-°F
Thermal Conductivity 0.600 W/m-K4.16 BTU-in/hr-ft²-°F
Melting Point 285 °C545 °F
Maximum Service Temperature, Air 220 - 240 °C428 - 464 °FUL temperature Index
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FASTM D648
Glass Transition Temp, Tg 88.0 °C190 °F
Flammability, UL94 5VA5VAV-0/5VA UL-94 Rating
Oxygen Index 53 %53 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Melt Temperature 304 - 343 °C579 - 649 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS); Molded
Chevron Phillips Ryton® R10-110BL Polyphenylene Sulfide Compound
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
Overview of materials for Polyphenylene Sulfide (PPS) Coating Resin

PZPSR51 / 58229

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.