VERSIFY™ 4301 Elastomer is a high melt flow rate resin suitable for a wide variety of applications and fabrication processes, including extrusion and injection molding. It is an excellent resin for films and soft compounds and is an excellent choice for PP modification. Main Characteristics: - High flow
- Superior Elasticity
- Excellent compatibility with PP
- Free flowing
Applications:- Soft compounds
- PP modification
- Blend component for thermoplastic elastomers
Complies with- EU, No 10/2011
- US FDA FCN 708
- US FDA 21 CFR 175.105 (c)(5)
Consult the regulations for complete details. |