MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow VERSIFY™ 4301 Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: VERSIFY™ 4301 Elastomer is a high melt flow rate resin suitable for a wide variety of applications and fabrication processes, including extrusion and injection molding. It is an excellent resin for films and soft compounds and is an excellent choice for PP modification.

Main Characteristics:

  • High flow
  • Superior Elasticity
  • Excellent compatibility with PP
  • Free flowing
Applications:
  • Soft compounds
  • PP modification
  • Blend component for thermoplastic elastomers
Complies with
  • EU, No 10/2011
  • US FDA FCN 708
  • US FDA 21 CFR 175.105 (c)(5)
Consult the regulations for complete details.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.868 g/cc0.0314 lb/in³ASTM D792
Melt Index of Compound 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
25 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8484Injection Molded, Aged two weeks prior to testing; ASTM D2240
Tensile Strength at Break 3.03 MPa439 psiInjection Molding, 50 mm/min, Aged two weeks prior to testing; ASTM D638
Tensile Strength, Yield 4.20 MPa609 psiInjection Molded, 50 mm/min; ASTM D638
Elongation at Yield 39 %39 %Injection Molded, 50 mm/min; ASTM D638
Tensile Modulus 0.00410 GPa0.595 ksi100% Secant (Injection Molded); ASTM D638
Flexural Modulus, 1% Secant 36.0 MPa5220 psiAged two weeks, (Compression Molded); ASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 51.0 °C124 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 2.2 %
@Thickness 2.00 mm
2.2 %
@Thickness 0.0787 in
Injection Molded; ASTM D1003
Gloss 73 %
@Thickness 2.00 mm
73 %
@Thickness 0.0787 in
45°, Injection Molded; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow VERSIFY™ 4200 Plastomer
Dow VERSIFY™ 2000 Plastomer
Dow VERSIFY™ 3000 Plastomer
Dow VERSIFY™ 3200 Elastomer
Dow VERSIFY™ 2200 Plastomer

PDOW2041 / 183688

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.