MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow VERSIFY™ 2200 Plastomer
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: VERSIFY™ 2200 Plastomer is a resin with a low melt flow rate making it suitable for blown film, blow molding, extrusion and thermoforming. It is an excellent sealant and is particularly suitable for use in BOPE structures. It has excellent compatibility with PP and is useful agent to bring softness and temperature performance.

Main Characteristics:

  • Pellet
  • Low Melt Flow Rate
  • Good sealant
  • Compatible with PP
  • Soft polypropylene
Applications:
  • Blown Film
  • Sealant
  • BOPE
  • Extrusion Applications
Complies with
  • EU, No 10/2011
  • US FDA FCN 909
  • US FDA 21 CFR 175.105(c)(5)
Consult the regulations for complete details.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.876 g/cc0.0316 lb/in³ASTM D792
Thickness 51.0 microns2.01 milFilm Thickness
Melt Index of Compound 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Crystallinity 21 %21 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 94
@Time 10.0 sec
94
@Time 0.00278 hour
Compression Molded; ASTM D2240
Hardness, Shore D 42
@Time 10.0 sec
42
@Time 0.00278 hour
Compression Molded; ASTM D2240
Tensile Strength at Break 20.5 MPa2970 psiCompression Molded; ASTM D638
Film Tensile Strength at Yield, MD 29.5 MPa
@Thickness 0.0510 mm
4280 psi
@Thickness 0.00201 in
ASTM D882
Film Tensile Strength at Yield, TD 26.3 MPa
@Thickness 0.0510 mm
3810 psi
@Thickness 0.00201 in
ASTM D882
Elongation at Break 690 %690 %50 mm/min, Compression Molded; ASTM D638
Flexural Modulus 0.0999 GPa
@Strain 2 %
14.5 ksi
@Strain 2 %
Secant (Compression Molded); ASTM D790
Secant Modulus, MD 0.0865 GPa
@Thickness 0.0510 mm
12.5 ksi
@Thickness 0.00201 in
2% Secant; ASTM D882
Secant Modulus, TD 0.0944 GPa
@Thickness 0.0510 mm
13.7 ksi
@Thickness 0.00201 in
2% Secant; ASTM D882
Elmendorf Tear Strength MD 590 g
@Thickness 0.0510 mm
590 g
@Thickness 0.00201 in
Method B; ASTM D1922
Elmendorf Tear Strength TD 1300 g
@Thickness 0.0510 mm
1300 g
@Thickness 0.00201 in
Method B; ASTM D1922
Film Tensile Strength at Break, MD 10.7 MPa
@Thickness 0.0510 mm
1550 psi
@Thickness 0.00201 in
ASTM D882
Film Tensile Strength at Break, TD 10.1 MPa
@Thickness 0.0510 mm
1460 psi
@Thickness 0.00201 in
ASTM D882
Heat Seal Strength Initiation Temperature  60.0 °C
@Thickness 0.0510 mm
140 °F
@Thickness 0.00201 in
Temperature at which 1 lb/in. (4.4 N/25.4 mm) heat seal strength is achieved
 80.0 °C
@Thickness 0.0508 mm
176 °F
@Thickness 0.00200 in
Ultimate
 
Thermal PropertiesMetricEnglishComments
Melting Point 82.2 °C180 °FDSC
Vicat Softening Point 63.0 °C145 °FASTM D1525
Glass Transition Temp, Tg -24.0 °C-11.2 °FDSC
 
Optical PropertiesMetricEnglishComments
Haze 4.8 %
@Thickness 39.4 mm
4.8 %
@Thickness 1.55 in
Injection Molded; ASTM D1003
Gloss  110 %
@Thickness 1.00 mm
110 %
@Thickness 0.0394 in
20°, Compression Molded, Gardner; ASTM D523
 128 %
@Thickness 1.00 mm
128 %
@Thickness 0.0394 in
60°, Compression Molded, Gardner; ASTM D523
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow VERSIFY™ 3200 Elastomer
Dow VERSIFY™ 2000 Plastomer
Dow VERSIFY™ 2300 Elastomer
Dow VERSIFY™ 3000 Plastomer
Dow VERSIFY™ 3300 Elastomer

PDOW2034 / 183681

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.