Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability. Information provided by Chevron Phillips Measured on 102mm x 102mm x 3.2 mm plaques, edge gated. |