MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Xtel® XE3035BL Polyphenylene Sulfide Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Xtel® XE3035BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.

Information provided by Chevron Phillips

Measured on 102mm x 102mm x 3.2 mm plaques, edge gated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ISO 1183A
Water Absorption 0.10 %0.10 %ASTM D-570
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 100 MPa14500 psiISO 527
Elongation at Yield 2.5 %2.5 %ISO 527
Flexural Strength 140 MPa20300 psiISO 178
Flexural Modulus 7.50 GPa1090 ksiISO 178
Compressive Strength 90.0 MPa13100 psiISO 604
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²ISO 180A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²19.0 ft-lb/in²ISO 180A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D-257
Insulation Resistance 1.00e+10 ohm
@Temperature 90.0 °C,
Time 173000 sec
1.00e+10 ohm
@Temperature 194 °F,
Time 48.0 hour
95% RH
Dielectric Constant  3.5
@Frequency 1000 Hz
3.5
@Frequency 1000 Hz
ASTM D-150
 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
ASTM D-150
Dielectric Strength 20.0 kV/mm508 kV/inASTM D-149
Dissipation Factor  0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D-150
 0.011
@Frequency 1e+6 Hz
0.011
@Frequency 1e+6 Hz
ASTM D-150
Arc Resistance 120 sec120 secASTM D-495
Comparative Tracking Index 150 V150 VUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.0 µm/m-°C
@Temperature 100 - 200 °C
5.56 µin/in-°F
@Temperature 212 - 392 °F
Axial; ISO 11359-2
 20.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
11.1 µin/in-°F
@Temperature -58.0 - 122 °F
Axial; ISO 11359-2
CTE, linear, Transverse to Flow  120 µm/m-°C
@Temperature -50.0 - 50.0 °C
66.7 µin/in-°F
@Temperature -58.0 - 122 °F
ISO 11359-2
 120 µm/m-°C
@Temperature 100 - 200 °C
66.7 µin/in-°F
@Temperature 212 - 392 °F
ISO 11359-2
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 315 - 345 °C599 - 653 °F
Mold Temperature 135 °C275 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy
Chevron Phillips Xtel® XE5300NA Polyphenylene Sulfide Alloy
Chevron Phillips Xtel® XE3200NA Polyphenylene Sulfide Alloy

PCHEVD257 / 20751

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.