MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultraform® H 4320 Q600 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Ultraform H4320 Q600 is an extrusion POM high molecular weight grade. This grade enables high extrusion rates with thick-walled product. It also exhibits high thermal stability and a low tendency to discolor.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ISO 1183
Water Absorption 0.80 %0.80 %ISO 62
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C/50% R.H.; ISO 62
Melt Flow 26 g/10 min
@Load 2.16 kg,
Temperature 190 °C
26 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 125 MPa18100 psi358/30; ISO 2039-1
Tensile Strength, Yield 63.0 MPa9140 psi50mm/min; ISO 527
Elongation at Break 31 %31 %50mm/min; ISO 527
Elongation at Yield 10 %10 %50mm/min; ISO 527
Modulus of Elasticity 2.60 GPa377 ksiISO 527
Izod Impact, Notched (ISO) 6.50 kJ/m²3.09 ft-lb/in²ISO 180/A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
Charpy Impact Unnotched 25.0 J/cm²119 ft-lb/in²ISO 179
 18.0 J/cm²
@Temperature -30.0 °C
85.7 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179
 0.550 J/cm²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Tensile Creep Modulus, 1000 hours 1300 MPa189000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
IEC 60250
 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mm1020 kV/inIEC 60243-1
Dissipation Factor  0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 600 V600 VTest Solution B; ICE 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 166 °C331 °FDIN 53765
Maximum Service Temperature, Air 100 °C212 °F
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75
Vicat Softening Point 150 °C302 °F(50 °C/h / 50N) - B/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °FInjection molding
Mold Temperature 60.0 - 120 °C140 - 248 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1500
NSF YesYesNSF Std. 51
 YesYesNSF Std. 61
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueExtrusion
ProcessingInjection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Semitron™ MDS 100 PEEK
BASF Ultraform® H 2320 006 Q600 POM
Mitsubishi Chemical Advanced Materials Semitron™ CMP LL5 PET Polyester
Mitsubishi Chemical Advanced Materials Semitron™ CMP XL20 PAI
Mitsubishi Chemical Advanced Materials Semitron™ ESd 225 POM Extruded, Static Dissipative Acetal

PBASF9100 / 84864

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.