System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Lehigh Technologies 200 Mesh Ground Reclaimed Whole Tire Rubber
Categories:
Other Engineering Material
;
Additive/Filler for Polymer
;
Polymer
;
Thermoset
;
Rubber or Thermoset Elastomer (TSE)
Material Notes:
A free flowing black powder produced from vulcanized rubber material
Information provided by Lehigh Technologies, LLC.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.14
g/cc
Particle Mesh Size
140
Mesh
0
170
Mesh
0
200
Mesh
0-10 %
Carbon Black Loading
26 - 38 %
Ash
8.0 - 12 %
Processing Properties
Original Value
Comments
Moisture Content
<= 0.50 %
Descriptive Properties
Acetone Extractables wt.%
8.0 - 22.0
Fiber Content Max wt.%
0.5
Loss on Heating
1
Metal Content Max wt.%
0.1
Natural Rubber wt.%
10.0 - 36.0
Rubber Hydrocarbon Content
42.0 - 47.0%
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
3M FV052 Tire Vinyl Label Products
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Lehigh Technologies 80 Mesh Ground Reclaimed Whole Tire Rubber
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)
Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
PLEHIG2 / 50566
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.