MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M FV052 Tire Vinyl Label Products
Categories: Polymer; Adhesive

Material Notes: 3M™ Tire Vinyl Label Products are white vinyl label stocks that offer durability and conformability. These vinyl labels utilize 3M™ Adhesive P1110, which is designed for labeling tires when used with tire wash. This adhesive exhibits high initial tack, yet resists edge bleed and cold flow.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 78.7 microns3.10 milLiner
 88.9 microns3.50 milFacestock
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.701 kN/m4.00 pli180° Peel, 12"/min., 1" wide sample; TLMI Method
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 68.0 °C154 °F
Minimum Service Temperature, Air 5.00 °C41.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 13.0 °C>= 55.4 °FApplication
 <= 43.0 °C<= 109 °FApplication
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive TypeP1110 Perm 26
Liner50# SC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lehigh Technologies 200 Mesh Ground Reclaimed Whole Tire Rubber
Lehigh Technologies 80 Mesh Ground Reclaimed Whole Tire Rubber
3M FV01460 Soft Clear Vinyl Label Products
Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Synthos BUNA™ SB 1502 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)

PMM33711 / 168458

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.