MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: BUNA™ CIS 132–Schkopau is a stereospecific butadiene with a high 1,4-cis content. It is manufactured by a solution process using an organo-metallic nickel catalyst which produces a consistent light coloured polymer with low ash content. BUNATM cis 132–Schkopau contains a non-staining stabilizer.

Application: BUNATM cis 132–Schkopau is widely used in the tire industry but also in the production of conveyor belts and other rubber articles which are exposed to high cyclical stress. It offers good abrasion resistance, high resilience, low hysteresis, and a low glass transition temperature. BUNATM cis 132–Schkopau offers excellent processability and may be blended with natural rubber and styrene butadiene (SBR), isoprene (IR), nitrile (NBR), or polychloroprene (CR) synthetic rubbers. Due to its non-staining stabilizer BUNATM cis 132–Schkopau is suitable for light-colored rubber articles also when compounded with selected thermoplastics.

Synthos acquired the synthetic rubber business from Trinseo in 2021.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³
Volatiles 0.24 %0.24 %1 hr at 105°C in a hot air oven, 5 g sample; ASTM D5668
Mooney Viscosity 45
@Temperature 100 °C
45
@Temperature 212 °F
MU, ML 1+4; ASTM D1646
Ash 0.010 %0.010 %ASTM D5667
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.4 MPa2520 psiCure: 45 min at 145°C; ASTM D412
Elongation at Break 490 %490 %ASTM D412
300% Modulus 9.10 MPa
@Strain 300 %
1320 psi
@Strain 300 %
ASTM D412
 
Descriptive Properties
Cis-1,4 content95 percentSM (FTIR)
Gel content3%SM
Rheometer11.6 mintc(90), ASTM D5289
 16.9 dNmMH, ASTM D5289
 2.7 dNmML, ASTM D5289
 5.9 mints2, 160°C, ASTM D5289
 8.0 mintc(50), ASTM D5289
Test Formulation0.9 PartAccelerator (TBBS),ASTM D3189
 1.75 PartsSulfur, ASTM D3189
 100 PartsPolymer, ASTM D3189
 15 PartsPlasticizer, ASTM D3189
 2 PartsStearic acid, ASTM D3189
 3 PartsZinc oxide, ASTM D3189
 60 PartsCarbon black IRB8, ASTM D3189

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR)
Dow SE BR-1220M Stereospecific high cis-1,4 Polybutadiene (BR)
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Nitriflex SB-1011 Styrene Butadiene Copolymer

PDWST235 / 142444

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.