MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lehigh Technologies 80 Mesh Ground Reclaimed Whole Tire Rubber
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: A free flowing black powder produced from vulcanized rubber material

Information provided by Lehigh Technologies, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/cc
Particle Mesh Size 60 Mesh60 Mesh0
 80 Mesh80 Mesh0-10 %
Carbon Black Loading 26 - 38 %26 - 38 %
Ash 8.0 - 12 %8.0 - 12 %
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %
 
Descriptive Properties
Acetone Extractables wt.%8.0 - 22.0
Fiber Content Max wt.%0.5
Metal Content Max wt.%0.1
Natural Rubber wt.%10.0 - 36.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M FV052 Tire Vinyl Label Products
Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Lehigh Technologies 200 Mesh Ground Reclaimed Whole Tire Rubber
Overview of materials for High Density Polyethylene (HDPE), Extruded
Synthos BUNA™ SB 1502 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)

PLEHIG0 / 50564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.