MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Firefly 800 Roller & Furnace Cladding Material
Categories: Ceramic

Material Notes: Firefly 800 is a beige asbestos-free material made from high-quality shot-free mineral wool and inert fillers. Rollers made of Firefly 800 are constructed to resist breakage in handling service. Firefly 800 exhibits excellent flame and heat resistance with virtually no dimensional changes. It has self-cleaning properties and has no shot or abrasive elements to scratch hot glass.

Applications

  • Furnace lining
  • Roller cladding material
  • Gaskets and seals

Advantages

  • Asbestos-free
  • Excellent thermal stability
  • High mechanical strength
  • Non-abrasive
  • Wet moldable

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.875 g/cc0.0316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  1.80 MPa
@Temperature 500 °C
261 psi
@Temperature 932 °F
 3.50 MPa
@Temperature 800 °C
508 psi
@Temperature 1470 °F
 4.00 MPa
@Temperature 23.0 °C
580 psi
@Temperature 73.4 °F
Compressive Strength 21.0 MPa3050 psi35-45%
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.110 - 0.150 W/m-K
@Temperature 50.0 - 400 °C
0.763 - 1.04 BTU-in/hr-ft²-°F
@Temperature 122 - 752 °F
Maximum Service Temperature, Air 1000 °C1830 °F
Shrinkage  0.25 %
@Temperature 1000 °C
0.25 %
@Temperature 1830 °F
Width
 0.89 %
@Temperature 1000 °C
0.89 %
@Temperature 1830 °F
Length
 1.9 %
@Temperature 1000 °C
1.9 %
@Temperature 1830 °F
Thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Firemaster Board 350 Thermal Ceramic
Pyrotek U-1 Compressible Board
Thermal Ceramics FireMaster Marine Blanket
Thermal Ceramics V-19 Block Insulation
Unifrax FyreWrap® Marine Blanket Insulation

CPYRO137 / 1859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.