MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Unifrax FyreWrap® Marine Blanket Insulation
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: FyreWrap® Marine Blanket from Unifrax is a totally inorganic, flexible, high-temperature insulation blanket specifically designed to provide passive fire protection for marine applications. The calcia, magnesia, silica chemistry is designed to enhance biosolubility. Unifrax's proprietary fiber spinning technology combined with mechanical needling of the fibers eliminates the need for binders in the product. This results in a material with high tensile strength and superior thermal and acoustical properties. Insulfrax Marine Blanket is chemically stable and its thermal properties are unaffected after exposure to water immersion or high humidity.

FyreWrap Marine Blanket provides fire protection insulation for a variety of rated assemblies on marine structures and vessels. Thin, lightweight systems combined with a flexible product form result in lower installation costs and significant weight savings. This offers builders and owners reduced structure weight, which may yield increased vessel speed, fuel savings and available payloads. FyreWrap Marine Blanket provides the following product features:

  • U.S. Coast Guard approved for steel and aluminum structures
  • Complies with SOLAS Safety Objectives and new IMO FTP Code fire test requirements; Res.A.754(18)
  • Fire Resisting Division for High Speed Craft (HSC); Res. MSC.45(65)
  • Fire protection structural insulation for bulkheads and decks
  • Significant weight savings versus mineral wool systems
  • Flexible blanket is easy to cut and install

Applications: FyreWrap Marine Blanket is utilized to insulate bulkheads and decks on passenger and vehile fast ferries, cruise ships, commercial and military vessels, and offshore oil platforms. Tested systems are in compliance with U.S. Coast Guard regulations, now defined under IMO Res.A.754(18). Typical applications include:

  • Steel bulkheads and decks
  • Aluminum bulkheads and decks, including extruded thin plate designs (min. 2mm thick)
  • Vehicle loading areas, engine rooms, storage areas, etc.
  • Various H-Rated offshore structures
  • Non-combustible insulation

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Loss On Ignition 0.00 %0.00 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 1260 °C2300 °F
 
Descriptive Properties
ASTM C136 Non-combustibilityPass
Temperature Grade (°C)1100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium AM100A-T4, Cast
Magnesium AM100A-T61, Sand Cast
Magnesium AM100A-F, Cast
Magnesium AS41XA-F, Die Cast
Magnesium AM60B-F, Die Cast

CUNIF115 / 97887

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.