MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Springflex Strip steel
Categories: Metal; Ferrous Metal; Austenitic; Ferritic; Stainless Steel

Material Notes: Sandvik Springflex is a duplex (austenitic-ferritic) stainless spring steel with very good spring properties and excellent corrosion resistance. Sandvik Springflex is characterized by:
  • Very good spring properties and fatigue resistance
  • High resistance to stress corrosion cracking (SCC) in chloride containing environments
  • High resistance to general corrosion, pitting and crevice corrosion
  • High tensile strength
  • High modulus of elasticity
Service temperature: -100 to 300°C (-150 to 570°F)

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1100 - 1900 MPa160000 - 276000 psiCold rolled
 1200 - 2200 MPa174000 - 319000 psiCold rolled and tempered, 450° C(840°F)/11h
Tensile Strength, Yield  1000 - 1700 MPa
@Strain 0.2 %
145000 - 247000 psi
@Strain 0.2 %
Cold rolled
 1150 - 2000 MPa
@Strain 0.2 %
167000 - 290000 psi
@Strain 0.2 %
Cold rolled and tempered, 450° C(840°F)/11h
Modulus of Elasticity 200 GPa29000 ksiCold rolled
 210 GPa30500 ksiCold rolled and tempered
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.00000740 ohm-cm
@Temperature 20.0 °C
0.00000740 ohm-cm
@Temperature 68.0 °F
 0.00000850 ohm-cm
@Temperature 100 °C
0.00000850 ohm-cm
@Temperature 212 °F
 0.00000960 ohm-cm
@Temperature 200 °C
0.00000960 ohm-cm
@Temperature 392 °F
 0.0000100 ohm-cm
@Temperature 300 °C
0.0000100 ohm-cm
@Temperature 572 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.0 µm/m-°C
@Temperature 20.0 - 100 °C
7.22 µin/in-°F
@Temperature 68.0 - 212 °F
 13.5 µm/m-°C
@Temperature 20.0 - 200 °C
7.50 µin/in-°F
@Temperature 68.0 - 392 °F
 14.0 µm/m-°C
@Temperature 20.0 - 300 °C
7.78 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
Thermal Conductivity  14.0 W/m-K
@Temperature 20.0 °C
97.2 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 16.0 W/m-K
@Temperature 100 °C
111 BTU-in/hr-ft²-°F
@Temperature 212 °F
 19.0 W/m-K
@Temperature 300 °C
132 BTU-in/hr-ft²-°F
@Temperature 572 °F
Maximum Service Temperature, Air 300 °C572 °F
Minimum Service Temperature, Air -100 °C-148 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 22 %22 %
Manganese, Mn 0.90 %0.90 %
Molybdenum, Mo 3.2 %3.2 %
Nickel, Ni 5.5 %5.5 %
Nitrogen, N 0.18 %0.18 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.50 %0.50 %
Sulfur, S <= 0.015 %<= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik 11R51 Strip steel
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 53% Cold Reduction + Aged 538°C (1000°F)/4hr/AC
Sandvik 13RM19 Strip Steel
Phynox Cobalt-Chromium-Nickel Alloy
ASTM A228 Steel (UNS K08500)

NSANDV5231 / 199795

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.