MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASTM A228 Steel (UNS K08500)
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; High Carbon Steel

Material Notes: Cold drawn. High tensile strength and uniform mechanical properties. Music wire springs are not recommended for service temperatures above 121°C (250°F).

Applications: High quality springs and wire forms subject to high stresses or requiring good fatigue properties.

Key Words: spring steel, music wire, AMS 5112, UNS K08500
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³Typical of ASTM Steel
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 41 - 6041 - 60
Tensile Strength, Yield  1590 - 1760 MPa
@Diameter 6.35 mm
231000 - 255000 psi
@Diameter 0.250 in
 1640 - 1820 MPa
@Diameter 5.26 mm
238000 - 264000 psi
@Diameter 0.207 in
 1690 - 1860 MPa
@Diameter 4.50 mm
245000 - 270000 psi
@Diameter 0.177 in
 1740 - 1920 MPa
@Diameter 3.81 mm
252000 - 278000 psi
@Diameter 0.150 in
 1770 - 1950 MPa
@Diameter 3.56 mm
257000 - 283000 psi
@Diameter 0.140 in
 1800 - 1990 MPa
@Diameter 3.18 mm
261000 - 289000 psi
@Diameter 0.125 in
 1870 - 2070 MPa
@Diameter 2.54 mm
271000 - 300000 psi
@Diameter 0.100 in
 1940 - 2150 MPa
@Diameter 2.00 mm
281000 - 312000 psi
@Diameter 0.0787 in
 2020 - 2230 MPa
@Diameter 1.60 mm
293000 - 323000 psi
@Diameter 0.0630 in
 2090 - 2310 MPa
@Diameter 1.30 mm
303000 - 335000 psi
@Diameter 0.0512 in
 2170 - 2410 MPa
@Diameter 1.00 mm
315000 - 350000 psi
@Diameter 0.0394 in
 2250 - 2490 MPa
@Diameter 0.810 mm
326000 - 361000 psi
@Diameter 0.0319 in
 2350 - 2600 MPa
@Diameter 0.610 mm
341000 - 377000 psi
@Diameter 0.0240 in
 2500 - 2760 MPa
@Diameter 0.400 mm
363000 - 400000 psi
@Diameter 0.0157 in
 2600 - 2880 MPa
@Diameter 0.300 mm
377000 - 418000 psi
@Diameter 0.0118 in
 2750 - 3040 MPa
@Diameter 0.200 mm
399000 - 441000 psi
@Diameter 0.00787 in
 3030 - 3340 MPa
@Diameter 0.100 mm
439000 - 484000 psi
@Diameter 0.00394 in
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.3130.313Calculated
Shear Modulus 80.0 GPa11600 ksi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.70 - 1.0 %0.70 - 1.0 %
Iron, Fe 97.8 - 99 %97.8 - 99 %
Manganese, Mn 0.20 - 0.60 %0.20 - 0.60 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si 0.10 - 0.30 %0.10 - 0.30 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A227 Steel Wire, Class I
304 Stainless Steel (UNS S30400); 1/2 Hard Bar, Plate, Sheet, and Strip
Overview of materials for High Carbon Steel
ASTM A232 Alloy Steel Wire
ASTM A229 Oil-tempered Steel Wire, Class I

MSASTMA228 / 14072

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.