MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ASTM A228 Steel (UNS K08500)
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; High Carbon Steel

Material Notes: Cold drawn. High tensile strength and uniform mechanical properties. Music wire springs are not recommended for service temperatures above 121°C (250°F).

Applications: High quality springs and wire forms subject to high stresses or requiring good fatigue properties.

Key Words: spring steel, music wire, AMS 5112, UNS K08500
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/ccTypical of ASTM Steel
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 41 - 60
Tensile Strength, Yield 1590 - 1760 MPa
@Diameter 6.35 mm
 1640 - 1820 MPa
@Diameter 5.26 mm
 1690 - 1860 MPa
@Diameter 4.50 mm
 1740 - 1920 MPa
@Diameter 3.81 mm
 1770 - 1950 MPa
@Diameter 3.56 mm
 1800 - 1990 MPa
@Diameter 3.18 mm
 1870 - 2070 MPa
@Diameter 2.54 mm
 1940 - 2150 MPa
@Diameter 2.00 mm
 2020 - 2230 MPa
@Diameter 1.60 mm
 2090 - 2310 MPa
@Diameter 1.30 mm
 2170 - 2410 MPa
@Diameter 1.00 mm
 2250 - 2490 MPa
@Diameter 0.810 mm
 2350 - 2600 MPa
@Diameter 0.610 mm
 2500 - 2760 MPa
@Diameter 0.400 mm
 2600 - 2880 MPa
@Diameter 0.300 mm
 2750 - 3040 MPa
@Diameter 0.200 mm
 3030 - 3340 MPa
@Diameter 0.100 mm
Modulus of Elasticity 210 GPa
Poissons Ratio 0.313Calculated
Shear Modulus 80.0 GPa
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.70 - 1.0 %
Iron, Fe 97.8 - 99 %
Manganese, Mn 0.20 - 0.60 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.10 - 0.30 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A227 Steel Wire, Class I
304 Stainless Steel (UNS S30400); 1/2 Hard Bar, Plate, Sheet, and Strip
Overview of materials for High Carbon Steel
ASTM A232 Alloy Steel Wire
ASTM A229 Oil-tempered Steel Wire, Class I

MSASTMA228 / 14072

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.