This Cobalt-Chromium-Nickel alloy also known as Elgiloy® gives a combination of high strength, ductility and good mechanical properties and is age hardenable. Phynox also has excellent fatigue life, corrosion resistance in numerous environments and is non-magnetic. This alloy is recommended where a high resistance to corrosion and / or low relaxation at temperatures up to 380°C are required. Applications include: - Springs
- Seal components
- Medical devices
- Components for watches
- Aerospace applications
- Petro-chemical applications
- Marine engineering
Information provided by Alloywire International. |
UNS R30003, AMS 5833; ISO 5832; AMS 5834; NACE MR0175 / ISO 15156-3 |