MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polyphenylene Ether, Molded
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.04 - 1.27 g/ccAverage value: 1.08 g/cc Grade Count:78
Water Absorption 0.000 - 0.500 %Average value: 0.108 % Grade Count:24
Moisture Absorption at Equilibrium 0.0600 - 0.900 %Average value: 0.224 % Grade Count:13
Water Absorption at Saturation 0.230 - 0.400 %Average value: 0.310 % Grade Count:3
Linear Mold Shrinkage 0.00400 - 0.0160 cm/cmAverage value: 0.00694 cm/cm Grade Count:62
Linear Mold Shrinkage, Transverse 0.00550 - 0.0100 cm/cmAverage value: 0.00700 cm/cm Grade Count:5
Melt Flow 0.100 - 96.0 g/10 minAverage value: 20.3 g/10 min Grade Count:34
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 82.0 - 84.0Average value: 83.3 Grade Count:3
Hardness, Rockwell R 110 - 119Average value: 116 Grade Count:14
Tensile Strength, Ultimate 34.5 - 90.0 MPaAverage value: 52.3 MPa Grade Count:47
 20.0 - 46.0 MPa
@Temperature 60.0 - 120 °C
Average value: 33.2 MPa Grade Count:2
Tensile Strength, Yield 34.5 - 76.0 MPaAverage value: 51.0 MPa Grade Count:46
Elongation at Break 2.00 - 140 %Average value: 48.1 % Grade Count:43
Elongation at Yield 3.00 - 45.0 %Average value: 13.4 % Grade Count:13
Modulus of Elasticity 2.00 - 5.70 GPaAverage value: 2.66 GPa Grade Count:13
Flexural Yield Strength 47.6 - 117 MPaAverage value: 75.6 MPa Grade Count:51
Flexural Modulus 1.76 - 2.94 GPaAverage value: 2.27 GPa Grade Count:67
 2.06 - 2.50 GPa
@Temperature 60.0 - 120 °C
Average value: 2.26 GPa Grade Count:2
Izod Impact, Notched 0.690 - 7.35 J/cmAverage value: 2.33 J/cm Grade Count:64
 0.540 - 1.90 J/cm
@Temperature -40.0 - -20.0 °C
Average value: 1.18 J/cm Grade Count:13
 0.784532 - 0.980665 J/cm
@Temperature -40.0 - -30.0 °C
Average value: 1.18 J/cm Grade Count:1
 0.784532 - 0.980665 J/cm
@Thickness 3.20 - 3.20 mm
Average value: 1.18 J/cm Grade Count:1
Izod Impact, Notched (ISO) 8.00 - 33.0 kJ/m²Average value: 16.4 kJ/m² Grade Count:4
 4.20 - 4.20 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 4.20 kJ/m² Grade Count:1
Charpy Impact Unnotched 4.50 J/cm² - NBAverage value: 18.8 J/cm² Grade Count:12
 30.0 J/cm² - NB
@Temperature -40.0 - -20.0 °C
Average value: 30.0 J/cm² Grade Count:3
Charpy Impact, Notched 1.00 - 4.50 J/cm²Average value: 2.07 J/cm² Grade Count:18
 1.20 - 1.20 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 1.20 J/cm² Grade Count:1
Gardner Impact 13.6 - 16.9 JAverage value: 16.3 J Grade Count:15
Tensile Impact Strength 42.0 - 268 kJ/m²Average value: 155 kJ/m² Grade Count:6
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+15 - 1.00e+17 ohm-cmAverage value: 9.59e+15 ohm-cm Grade Count:22
Surface Resistance 1000 - 1.00e+15 ohmAverage value: 4.25e+14 ohm Grade Count:12
Dielectric Constant 2.00 - 3.50Average value: 2.53 Grade Count:14
Dielectric Strength 19.0 - 50.0 kV/mmAverage value: 30.8 kV/mm Grade Count:13
Dissipation Factor 0.000100 - 0.0200Average value: 0.00293 Grade Count:14
Comparative Tracking Index 85.0 - 400 VAverage value: 237 V Grade Count:12
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 - 100 µm/m-°CAverage value: 68.6 µm/m-°C Grade Count:25
CTE, linear, Transverse to Flow 50.0 µm/m-°CAverage value: 50.0 µm/m-°C Grade Count:7
Melting Point 181 - 290 °CAverage value: 217 °C Grade Count:3
Maximum Service Temperature, Air 85.0 - 150 °CAverage value: 110 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 87.8 - 190 °CAverage value: 131 °C Grade Count:40
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 260 °CAverage value: 114 °C Grade Count:69
Vicat Softening Point 95.0 - 216 °CAverage value: 146 °C Grade Count:19
Flammability, UL94 HB - 5VAGrade Count:56
Oxygen Index 22.0 - 30.0 %Average value: 26.0 % Grade Count:3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 193 - 300 °CAverage value: 256 °C Grade Count:14
Melt Temperature 204 - 316 °CAverage value: 277 °C Grade Count:28
Mold Temperature 50.0 - 104 °CAverage value: 81.0 °C Grade Count:36
Drying Temperature 55.0 - 120 °CAverage value: 99.0 °C Grade Count:39
Vent Depth 0.00381 cmAverage value: 0.00381 cm Grade Count:11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetherimide (PEI)
Overview of materials for Polystyrene, Molded, Unreinforced
Overview of materials for Polysulfone (PSU)
Overview of materials for Polyethersulfone (PES)
Overview of materials for Polyimide

O4400 / 78318

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.