MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyethersulfone (PES)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 - 1.85 g/cc0.0437 - 0.0668 lb/in³Average value: 1.49 g/cc Grade Count:239
Filler Content 5.00 - 40.0 %5.00 - 40.0 %Average value: 20.4 % Grade Count:56
Water Absorption 0.100 - 2.20 %0.100 - 2.20 %Average value: 0.614 % Grade Count:134
Moisture Absorption at Equilibrium 0.0200 - 1.00 %0.0200 - 1.00 %Average value: 0.356 % Grade Count:59
Additive Loading 10.0 - 40.0 %10.0 - 40.0 %Average value: 27.3 % Grade Count:13
Particle Size 45.0 - 250 µm45.0 - 250 µmAverage value: 182 µm Grade Count:3
Viscosity 80.0 - 5000 cP80.0 - 5000 cPAverage value: 851 cP Grade Count:13
 10.0 - 20.0 cP
@Temperature 345 - 345 °C
10.0 - 20.0 cP
@Temperature 653 - 653 °F
Average value: 15.0 cP Grade Count:1
 10.0 - 20.0 cP
@Load 10.0 - 10.0 kg
10.0 - 20.0 cP
@Load 22.0 - 22.0 lb
Average value: 15.0 cP Grade Count:1
Viscosity Test 56.0 - 66.0 cm³/g0.560 - 0.660 dl/gAverage value: 57.4 cm³/g Grade Count:9
Viscosity Number 48.0 - 82.0 cm³/g0.480 - 0.820 dl/gAverage value: 60.0 cm³/g Grade Count:7
Linear Mold Shrinkage 0.000500 - 0.0100 cm/cm0.000500 - 0.0100 in/inAverage value: 0.00405 cm/cm Grade Count:208
Linear Mold Shrinkage, Transverse 0.00250 - 0.00950 cm/cm0.00250 - 0.00950 in/inAverage value: 0.00658 cm/cm Grade Count:48
Melt Flow 4.00 - 150 g/10 min4.00 - 150 g/10 minAverage value: 38.8 g/10 min Grade Count:46
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 76.0 - 98.076.0 - 98.0Average value: 92.5 Grade Count:4
Hardness, Rockwell R 98.0 - 12798.0 - 127Average value: 121 Grade Count:41
Ball Indentation Hardness 154 - 227 MPa22300 - 32900 psiAverage value: 178 MPa Grade Count:13
Tensile Strength, Ultimate 56.5 - 325 MPa8190 - 47100 psiAverage value: 116 MPa Grade Count:199
 10.0 - 135 MPa
@Temperature 60.0 - 150 °C
1450 - 19600 psi
@Temperature 140 - 302 °F
Average value: 94.0 MPa Grade Count:4
Tensile Strength, Yield 65.5 - 221 MPa9500 - 32000 psiAverage value: 109 MPa Grade Count:50
 50.0 - 75.0 MPa
@Temperature 60.0 - 140 °C
7250 - 10900 psi
@Temperature 140 - 284 °F
Average value: 63.3 MPa Grade Count:1
Elongation at Break 0.450 - 100 %0.450 - 100 %Average value: 6.06 % Grade Count:193
 2.10 - 20.0 %
@Temperature 60.0 - 150 °C
2.10 - 20.0 %
@Temperature 140 - 302 °F
Average value: 28.3 % Grade Count:4
Elongation at Yield 0.189 - 6.90 %0.189 - 6.90 %Average value: 2.85 % Grade Count:52
 2.50 - 5.50 %
@Temperature 60.0 - 150 °C
2.50 - 5.50 %
@Temperature 140 - 302 °F
Average value: 3.85 % Grade Count:3
Modulus of Elasticity 2.00 - 36.6 GPa290 - 5300 ksiAverage value: 7.46 GPa Grade Count:208
 2.25 - 10.0 GPa
@Temperature 50.0 - 200 °C
326 - 1450 ksi
@Temperature 122 - 392 °F
Average value: 7.57 GPa Grade Count:8
Flexural Yield Strength 2.60 - 310 MPa377 - 45000 psiAverage value: 171 MPa Grade Count:202
Flexural Modulus 2.28 - 24.1 GPa330 - 3500 ksiAverage value: 7.19 GPa Grade Count:206
Flexural Strain at Break 1.40 - 3.80 %1.40 - 3.80 %Average value: 2.85 % Grade Count:4
Compressive Yield Strength 95.8 - 241 MPa13900 - 35000 psiAverage value: 133 MPa Grade Count:27
Fatigue Strength  5.00 - 43.0 MPa
@# of Cycles 10000 - 1.00e+7
725 - 6240 psi
@# of Cycles 10000 - 1.00e+7
Average value: 20.7 MPa Grade Count:2
 5.00 - 43.0 MPa
@Temperature 180 - 180 °C
725 - 6240 psi
@Temperature 356 - 356 °F
Average value: 20.7 MPa Grade Count:2
Shear Modulus 0.200 - 1.00 GPa
@Temperature 50.0 - 225 °C
29.0 - 145 ksi
@Temperature 122 - 437 °F
Average value: 0.762 GPa Grade Count:8
Izod Impact 42.0 - 96.0 J31.0 - 70.8 ft-lbAverage value: 60.8 J Grade Count:20
Izod Impact, Notched 0.214 - 2.14 J/cm0.400 - 4.00 ft-lb/inAverage value: 0.686 J/cm Grade Count:162
Izod Impact, Unnotched 1.87 - 5340 J/cm3.50 - 10000 ft-lb/inAverage value: 6.07 J/cm Grade Count:120
Izod Impact, Notched (ISO) 5.00 - 15.7 kJ/m²2.38 - 7.49 ft-lb/in²Average value: 7.22 kJ/m² Grade Count:56
 5.00 - 14.7 kJ/m²
@Temperature -30.0 - 120 °C
2.38 - 6.99 ft-lb/in²
@Temperature -22.0 - 248 °F
Average value: 7.87 kJ/m² Grade Count:11
Izod Impact, Unnotched (ISO) 6.50 kJ/m² - NB3.09 ft-lb/in² - NBAverage value: 39.6 kJ/m² Grade Count:41
 42.0 - 59.0 kJ/m²
@Temperature -25.0 - 120 °C
20.0 - 28.1 ft-lb/in²
@Temperature -13.0 - 248 °F
Average value: 52.7 kJ/m² Grade Count:1
Charpy Impact Unnotched 1.50 J/cm² - NB7.14 ft-lb/in² - NBAverage value: 3.59 J/cm² Grade Count:27
 2.50 J/cm² - NB
@Temperature -30.0 - -20.0 °C
11.9 ft-lb/in² - NB
@Temperature -22.0 - -4.00 °F
Average value: 3.88 J/cm² Grade Count:14
Charpy Impact, Notched 0.350 - 1.00 J/cm²1.67 - 4.76 ft-lb/in²Average value: 0.680 J/cm² Grade Count:29
 0.250 - 0.800 J/cm²
@Temperature -30.0 - -20.0 °C
1.19 - 3.81 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 0.654 J/cm² Grade Count:14
Tensile Impact Strength 70.0 - 336 kJ/m²33.3 - 160 ft-lb/in²Average value: 247 kJ/m² Grade Count:3
Dart Drop, Total Energy 4.00 - 16.0 J2.95 - 11.8 ft-lbAverage value: 10.8 J Grade Count:16
Falling Dart Impact 4.20 - 12.8 J3.10 - 9.44 ft-lbAverage value: 9.27 J Grade Count:4
Instrumented Impact Total Energy 2.36 - 4.16 J1.74 - 3.07 ft-lbAverage value: 2.92 J Grade Count:4
Coefficient of Friction 0.200 - 0.5200.200 - 0.520Average value: 0.413 Grade Count:11
Coefficient of Friction, Static 0.200 - 0.5700.200 - 0.570Average value: 0.365 Grade Count:11
Tensile Creep Modulus, 1000 hours 2700 - 8300 MPa392000 - 1.20e+6 psiAverage value: 3760 MPa Grade Count:8
K (wear) Factor 8.06 - 342 x 10-8 mm³/N-M4.00 - 170 x 10-10 in³-min/ft-lb-hrAverage value: 124 x 10-8 mm³/N-M Grade Count:10
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.90 - 1.00e+17 ohm-cm1.90 - 1.00e+17 ohm-cmAverage value: 9.06e+15 ohm-cm Grade Count:141
Surface Resistance 7.80 - 1.00e+15 ohm7.80 - 1.00e+15 ohmAverage value: 1.00e+14 ohm Grade Count:42
Static Decay 0.500 - 2.00 sec0.500 - 2.00 secAverage value: 1.58 sec Grade Count:12
Dielectric Constant 3.06 - 4.303.06 - 4.30Average value: 3.71 Grade Count:65
Dielectric Strength 8.00 - 181 kV/mm203 - 4600 kV/inAverage value: 23.0 kV/mm Grade Count:76
Dissipation Factor 0.00100 - 0.01400.00100 - 0.0140Average value: 0.00467 Grade Count:64
Arc Resistance 50.0 - 179 sec50.0 - 179 secAverage value: 83.5 sec Grade Count:23
Comparative Tracking Index 100 - 250 V100 - 250 VAverage value: 126 V Grade Count:18
Hot Wire Ignition, HWI 7.00 - 119 sec7.00 - 119 secAverage value: 39.9 sec Grade Count:3
High Amp Arc Ignition, HAI 60.0 - 120 arcs60.0 - 120 arcsAverage value: 113 arcs Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.00 - 59.0 µm/m-°C2.22 - 32.8 µin/in-°FAverage value: 38.5 µm/m-°C Grade Count:114
 4.00 - 60.0 µm/m-°C
@Temperature -26.0 - 180 °C
2.22 - 33.3 µin/in-°F
@Temperature -14.8 - 356 °F
Average value: 37.2 µm/m-°C Grade Count:12
 26.0 - 34.0 µm/m-°C
@Temperature 75.0 - 175 °C
14.4 - 18.9 µin/in-°F
@Temperature 167 - 347 °F
Average value: 37.2 µm/m-°C Grade Count:1
 26.0 - 34.0 µm/m-°C
@Thickness 2.00 - 4.00 mm
14.4 - 18.9 µin/in-°F
@Thickness 0.0787 - 0.157 in
Average value: 37.2 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 20.0 - 93.6 µm/m-°C11.1 - 52.0 µin/in-°FAverage value: 44.0 µm/m-°C Grade Count:23
 19.5 - 25.0 µm/m-°C
@Temperature 75.0 - 175 °C
10.8 - 13.9 µin/in-°F
@Temperature 167 - 347 °F
Average value: 22.3 µm/m-°C Grade Count:1
 19.5 - 25.0 µm/m-°C
@Thickness 2.00 - 4.00 mm
10.8 - 13.9 µin/in-°F
@Thickness 0.0787 - 0.157 in
Average value: 22.3 µm/m-°C Grade Count:1
Specific Heat Capacity 0.913 - 1.00 J/g-°C0.218 - 0.239 BTU/lb-°FAverage value: 0.971 J/g-°C Grade Count:3
Thermal Conductivity 0.163 - 5.99 W/m-K1.13 - 41.6 BTU-in/hr-ft²-°FAverage value: 0.473 W/m-K Grade Count:29
Maximum Service Temperature, Air 180 - 220 °C356 - 428 °FAverage value: 199 °C Grade Count:26
Deflection Temperature at 0.46 MPa (66 psi) 160 - 225 °C320 - 437 °FAverage value: 214 °C Grade Count:69
Deflection Temperature at 1.8 MPa (264 psi) 146 - 228 °C295 - 442 °FAverage value: 208 °C Grade Count:217
Vicat Softening Point 210 - 220 °C410 - 428 °FAverage value: 218 °C Grade Count:10
Glass Transition Temp, Tg 158 - 228 °C316 - 442 °FAverage value: 222 °C Grade Count:39
Decomposition Temperature 400 °C752 °FAverage value: 400 °C Grade Count:9
UL RTI, Electrical 180 - 190 °C356 - 374 °FAverage value: 183 °C Grade Count:21
UL RTI, Mechanical with Impact 170 - 190 °C338 - 374 °FAverage value: 181 °C Grade Count:16
UL RTI, Mechanical without Impact 180 - 190 °C356 - 374 °FAverage value: 186 °C Grade Count:14
Flammability, UL94 V-2 - 5VAV-2 - 5VAGrade Count:156
Oxygen Index 30.0 - 49.0 %30.0 - 49.0 %Average value: 40.2 % Grade Count:19
Glow Wire Test 825 - 960 °C1520 - 1760 °FAverage value: 902 °C Grade Count:4
Ignition Temperature 500 - 600 °C932 - 1110 °FAverage value: 580 °C Grade Count:9
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.63 - 1.681.63 - 1.68Average value: 1.65 Grade Count:7
Transmission, Visible 30.0 - 90.0 %30.0 - 90.0 %Average value: 79.8 % Grade Count:9
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 366 °C176 - 690 °FAverage value: 297 °C Grade Count:40
Nozzle Temperature 340 - 390 °C644 - 734 °FAverage value: 357 °C Grade Count:6
Adapter Temperature 300 - 371 °C572 - 700 °FAverage value: 338 °C Grade Count:8
Die Temperature 300 - 371 °C572 - 700 °FAverage value: 338 °C Grade Count:8
Melt Temperature 288 - 410 °C550 - 770 °FAverage value: 364 °C Grade Count:167
Mold Temperature 79.4 - 200 °C175 - 392 °FAverage value: 152 °C Grade Count:190
Drying Temperature 110 - 180 °C230 - 356 °FAverage value: 149 °C Grade Count:158
Moisture Content 0.0200 - 0.0500 %0.0200 - 0.0500 %Average value: 0.0407 % Grade Count:74
Dew Point -31.7 °C-25.0 °FAverage value: -31.7 °C Grade Count:61
Injection Pressure 3.45 - 103 MPa500 - 15000 psiAverage value: 84.5 MPa Grade Count:92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetherimide (PEI)
Overview of materials for Polysulfone (PSU)
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
BASF Ultrason® E 1010 PES
Overview of materials for Polyimide

O3700 / 77783

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.