Physical Properties | Metric | English | Comments |
---|
Density | 0.00545 - 1.95 g/cc | 0.000197 - 0.0704 lb/in³ |
Filler Content | 0.000 - 40.0 % | 0.000 - 40.0 % |
Water Absorption | 0.0400 - 1.86 % | 0.0400 - 1.86 % |
| 0.260 - 3.15 % @Temperature 50.0 - 80.0 °C | 0.260 - 3.15 % @Temperature 122 - 176 °F |
| 0.300 - 3.29 % @Temperature 50.0 - 80.0 °C | 0.300 - 3.29 % @Temperature 122 - 176 °F |
| 0.300 - 3.29 % @Time 86400 - 173000 sec | 0.300 - 3.29 % @Time 24.0 - 48.0 hour |
Moisture Absorption at Equilibrium | 0.0200 - 3.90 % | 0.0200 - 3.90 % |
Water Absorption at Saturation | 0.420 - 3.80 % | 0.420 - 3.80 % |
| 2.30 - 4.17 % @Temperature 80.0 - 80.0 °C | 2.30 - 4.17 % @Temperature 176 - 176 °F |
Viscosity | 8.00 - 16.0 cP @Temperature 360 - 360 °C | 8.00 - 16.0 cP @Temperature 680 - 680 °F |
| 8.00 - 16.0 cP @Load 5.00 - 5.00 kg | 8.00 - 16.0 cP @Load 11.0 - 11.0 lb |
Thickness | 5.00 - 127 microns | 0.197 - 5.00 mil |
Linear Mold Shrinkage | 0.000100 - 0.0140 cm/cm | 0.000100 - 0.0140 in/in |
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0140 cm/cm | 0.00500 - 0.0140 in/in |
Melt Flow | 2.00 - 37.0 g/10 min | 2.00 - 37.0 g/10 min |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Rockwell E | 20.0 - 91.0 | 20.0 - 91.0 |
Hardness, Rockwell M | 20.0 - 125 | 20.0 - 125 |
Hardness, Rockwell R | 123 - 129 | 123 - 129 |
Hardness, Shore D | 65.0 - 93.0 | 65.0 - 93.0 |
Ball Indentation Hardness | 138 - 345 MPa | 20000 - 50000 psi |
Tensile Strength, Ultimate | 0.0480 - 345 MPa | 6.96 - 50000 psi |
| 23.0 - 324.054 MPa @Temperature 150 - 260 °C | 3340 - 47000.1 psi @Temperature 302 - 500 °F |
Tensile Strength, Yield | 15.0 - 230 MPa | 2180 - 33300 psi |
| 27.579 - 141.343 MPa @Temperature 149 - 260 °C | 4000.0 - 20500.0 psi @Temperature 300 - 500 °F |
Elongation at Break | 0.350 - 200 % | 0.350 - 200 % |
| 1.70 - 90.0 % @Temperature 150 - 260 °C | 1.70 - 90.0 % @Temperature 302 - 500 °F |
Elongation at Yield | 2.00 - 90.0 % | 2.00 - 90.0 % |
| 4.00 - 90.0 % @Temperature 149 - 149 °C | 4.00 - 90.0 % @Temperature 300 - 300 °F |
Modulus of Elasticity | 0.107 - 46.9 GPa | 15.5 - 6800 ksi |
| 1.03421 - 3.71627 GPa @Temperature 260 - 260 °C | 150.002 - 539.008 ksi @Temperature 500 - 500 °F |
Flexural Yield Strength | 24.8 - 490 MPa | 3600 - 71000 psi |
| 20.6843 - 344.738 MPa @Temperature 149 - 260 °C | 3000.01 - 50000.1 psi @Temperature 300 - 500 °F |
Flexural Modulus | 1.38 - 40.0 GPa | 200 - 5800 ksi |
| 0.0102 - 30.3 GPa @Temperature 149 - 300 °C | 1.48 - 4390 ksi @Temperature 300 - 572 °F |
Flexural Strain at Break | 1.30 - 5.40 % | 1.30 - 5.40 % |
Flexural Strain at Yield | 1.40 - 7.90 % | 1.40 - 7.90 % |
Compressive Strain at Break | 12.0 - 54.0 % | 12.0 - 54.0 % |
| 21.0 - 31.0 % @Temperature 260 - 260 °C | 21.0 - 31.0 % @Temperature 500 - 500 °F |
Compressive Yield Strength | 0.00217 - 570 MPa | 0.315 - 82700 psi |
| 71.0 - 414 MPa @Temperature 149 - 260 °C | 10300 - 60000 psi @Temperature 300 - 500 °F |
| 96.0 - 172 MPa @Temperature 260 - 260 °C | 13900 - 24900 psi @Temperature 500 - 500 °F |
| 96.0 - 172 MPa @Strain 10.0 - 10.0 % | 13900 - 24900 psi @Strain 10.0 - 10.0 % |
Compressive Modulus | 0.00164 - 6.19 GPa | 0.238 - 898 ksi |
| 1.663 - 2.997 GPa @Temperature 260 - 260 °C | 241.2 - 434.7 ksi @Temperature 500 - 500 °F |
Poissons Ratio | 0.250 - 0.410 | 0.250 - 0.410 |
| 0.320 - 0.320 @Temperature 190 - 190 °C | 0.320 - 0.320 @Temperature 374 - 374 °F |
Fatigue Strength | 16.5474 - 26.2001 MPa @# of Cycles 1000 - 1.00e+7 | 2400.00 - 3800.01 psi @# of Cycles 1000 - 1.00e+7 |
| 16.5474 - 26.2001 MPa @Temperature 260 - 260 °C | 2400.00 - 3800.01 psi @Temperature 500 - 500 °F |
Shear Strength | 81.4 - 110 MPa | 11800 - 16000 psi |
| 60.8 - 78.5 MPa @Temperature 150 - 150 °C | 8820 - 11400 psi @Temperature 302 - 302 °F |
Izod Impact | 25.0 - 69.0 J | 18.4 - 50.9 ft-lb |
| 38.0 - 74.0 J @Temperature -30.0 - -30.0 °C | 28.0 - 54.6 ft-lb @Temperature -22.0 - -22.0 °F |
Izod Impact, Notched | 0.0700 - 9.20 J/cm | 0.131 - 17.2 ft-lb/in |
Izod Impact, Unnotched | 0.900 - 5340 J/cm | 1.69 - 10000 ft-lb/in |
Izod Impact, Notched (ISO) | 0.0430 - 27.0 kJ/m² | 0.0205 - 12.8 ft-lb/in² |
| 4.00 - 5.00 kJ/m² @Temperature -30.0 - -30.0 °C | 1.90 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Izod Impact, Unnotched (ISO) | 0.320 kJ/m² - NB | 0.152 ft-lb/in² - NB |
| 147 kJ/m² - NB @Temperature -30.0 - -30.0 °C | 69.9 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Charpy Impact Unnotched | 0.540 - 1000 J/cm² | 2.57 - 4760 ft-lb/in² |
| 999.9 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C | 4759 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Charpy Impact, Notched | 0.110 - 1.60 J/cm² | 0.524 - 7.61 ft-lb/in² |
Dart Drop, Total Energy | 33.0 J | 24.3 ft-lb |
Coefficient of Friction | 0.0600 - 0.490 | 0.0600 - 0.490 |
Coefficient of Friction, Static | 0.200 - 0.350 | 0.200 - 0.350 |
K Factor (Wear Factor) | 0.400 - 13.1 | 0.400 - 13.1 |
K (wear) Factor | 20.1 - 568 x 10-8 mm³/N-M | 10.0 - 282 x 10-10 in³-min/ft-lb-hr |
Limiting Pressure Velocity | 0.525 - 12.0 MPa-m/sec | 15000 - 343000 psi-ft/min |
Compression Set | 12.5 - 98.0 % | 12.5 - 98.0 % |
|
Electrical Properties | Metric | English | Comments |
---|
Electrical Resistivity | 0.100 - 4.00e+19 ohm-cm | 0.100 - 4.00e+19 ohm-cm |
Surface Resistance | 0.100 - 1.00e+18 ohm | 0.100 - 1.00e+18 ohm |
Dielectric Constant | 1.11 - 62.0 | 1.11 - 62.0 |
Dielectric Strength | 3.00 - 305 kV/mm | 76.2 - 7760 kV/in |
Dissipation Factor | 0.000900 - 0.310 | 0.000900 - 0.310 |
Dielectric Loss Index | 0.00180 - 0.0106 | 0.00180 - 0.0106 |
Comparative Tracking Index | 125 - 399 V | 125 - 399 V |
Hot Wire Ignition, HWI | 30.0 - 120 sec | 30.0 - 120 sec |
High Amp Arc Ignition, HAI | 0.000 - 15.0 arcs | 0.000 - 15.0 arcs |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 5.40 - 63.0 µm/m-°C | 3.00 - 35.0 µin/in-°F |
| 0.234 - 144 µm/m-°C @Temperature 15.6 - 400 °C | 0.130 - 80.0 µin/in-°F @Temperature 60.0 - 752 °F |
CTE, linear, Transverse to Flow | 6.00 - 55.0 µm/m-°C | 3.33 - 30.6 µin/in-°F |
| 36.0 - 70.0 µm/m-°C @Temperature 50.0 - 300 °C | 20.0 - 38.9 µin/in-°F @Temperature 122 - 572 °F |
Specific Heat Capacity | 0.920 - 1.24 J/g-°C | 0.220 - 0.296 BTU/lb-°F |
| 0.895376 - 1.42256 J/g-°C @Temperature 60.0 - 300 °C | 0.214000 - 0.340000 BTU/lb-°F @Temperature 140 - 572 °F |
Thermal Conductivity | 0.0330 - 1.73 W/m-K | 0.229 - 12.0 BTU-in/hr-ft²-°F |
| 0.220 - 2.05 W/m-K @Temperature 40.0 - 300 °C | 1.53 - 14.2 BTU-in/hr-ft²-°F @Temperature 104 - 572 °F |
Melting Point | 247 - 388 °C | 477 - 730 °F |
Maximum Service Temperature, Air | 200 - 395 °C | 392 - 743 °F |
Hot Ball Pressure Test | 125 °C | 257 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 215 - 377 °C | 419 - 711 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 196 - 470 °C | 385 - 878 °F |
Vicat Softening Point | 221 - 260 °C | 430 - 500 °F |
Minimum Service Temperature, Air | -240 - -20.0 °C | -400 - -4.00 °F |
Glass Transition Temp, Tg | -20.0 - 385 °C | -4.00 - 725 °F |
Decomposition Temperature | 431 - 570 °C | 808 - 1060 °F |
UL RTI, Electrical | 50.0 - 160 °C | 122 - 320 °F |
UL RTI, Mechanical with Impact | 50.0 - 130 °C | 122 - 266 °F |
UL RTI, Mechanical without Impact | 50.0 - 160 °C | 122 - 320 °F |
Flammability, UL94 | V-0 - 5VA | V-0 - 5VA |
Flame Spread Index | 0.000 - 5.00 | 0.000 - 5.00 |
Oxygen Index | 30.0 - 53.0 % | 30.0 - 53.0 % |
Glow Wire Test | 850 - 960 °C | 1560 - 1760 °F |
|
Optical Properties | Metric | English | Comments |
---|
Haze | 0.100 - 2.00 % | 0.100 - 2.00 % |
Transmission, Visible | 58.0 - 91.6 % | 58.0 - 91.6 % |
|
Processing Properties | Metric | English | Comments |
---|
Processing Temperature | 371 - 420 °C | 700 - 788 °F |
Nozzle Temperature | 375 - 405 °C | 707 - 761 °F |
Melt Temperature | 370 - 416 °C | 698 - 780 °F |
Mold Temperature | 135 - 232 °C | 275 - 450 °F |
Drying Temperature | 150 - 204 °C | 302 - 400 °F |
Moisture Content | 0.0100 % | 0.0100 % |
Dew Point | -40.0 °C | -40.0 °F |
Injection Pressure | 138 - 193 MPa | 20000 - 28000 psi |
Vent Depth | 0.00250 - 0.00760 cm | 0.000984 - 0.00299 in |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.