| Physical Properties | Metric | English | Comments |
|---|
| Density | 1.26 - 1.72 g/cc | 0.0454 - 0.0621 lb/in³ |
| Filler Content | 0.000 % | 0.000 % |
| Water Absorption | 0.0200 - 0.500 % | 0.0200 - 0.500 % |
| Moisture Absorption at Equilibrium | 0.0200 - 0.500 % | 0.0200 - 0.500 % |
| Water Absorption at Saturation | 0.0700 - 1.65 % | 0.0700 - 1.65 % |
| 0.550 - 0.560 % @Temperature 100 - 100 °C | 0.550 - 0.560 % @Temperature 212 - 212 °F |
| Particle Size | 10.0 - 550 µm | 10.0 - 550 µm |
| Viscosity | 90000 - 500000 cP @Temperature 400 - 400 °C | 90000 - 500000 cP @Temperature 752 - 752 °F |
| 1120 - 1120 cP @Temperature 380 - 380 °C | 1120 - 1120 cP @Temperature 716 - 716 °F |
| | 1120 - 1120 cP @Frequency 100 - 100 Hz | 1120 - 1120 cP @Frequency 100 - 100 Hz |
| Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in |
| Linear Mold Shrinkage, Transverse | 0.00110 - 0.0200 cm/cm | 0.00110 - 0.0200 in/in |
| Melt Flow | 0.260 - 182 g/10 min | 0.260 - 182 g/10 min |
| Spiral Flow | 11.0 - 70.0 cm | 4.33 - 27.6 in |
| 12.5 - 63.0 cm @Temperature 375 - 395 °C | 4.92 - 24.8 in @Temperature 707 - 743 °F |
| | 12.5 - 63.0 cm @Thickness 1.00 - 3.00 mm | 4.92 - 24.8 in @Thickness 0.0394 - 0.118 in |
| Ash | 3.60 - 25.4 % | 3.60 - 25.4 % |
| |
| Mechanical Properties | Metric | English | Comments |
|---|
| Hardness, Rockwell M | 85.0 - 109 | 85.0 - 109 |
| Hardness, Rockwell R | 105 - 126 | 105 - 126 |
| Hardness, Shore D | 62.0 - 94.0 | 62.0 - 94.0 |
| Ball Indentation Hardness | 90.0 - 250 MPa | 13100 - 36300 psi |
| Tensile Strength, Ultimate | 48.0 - 265 MPa | 6960 - 38400 psi |
| 25.0 - 80.0 MPa @Temperature 60.0 - 150 °C | 3630 - 11600 psi @Temperature 140 - 302 °F |
| Tensile Strength, Yield | 11.0 - 125 MPa | 1600 - 18200 psi |
| Elongation at Break | 1.70 - 110 % | 1.70 - 110 % |
| 30.0 - 45.0 % @Temperature 60.0 - 150 °C | 30.0 - 45.0 % @Temperature 140 - 302 °F |
| Elongation at Yield | 3.60 - 45.0 % | 3.60 - 45.0 % |
| 5.00 - 8.00 % @Temperature 60.0 - 150 °C | 5.00 - 8.00 % @Temperature 140 - 302 °F |
| Modulus of Elasticity | 2.14 - 8.27 GPa | 310 - 1200 ksi |
| 3.00 - 3.70 GPa @Temperature 60.0 - 150 °C | 435 - 537 ksi @Temperature 140 - 302 °F |
| Flexural Yield Strength | 86.2 - 380 MPa | 12500 - 55100 psi |
| 9.00 - 90.0 MPa @Temperature 125 - 275 °C | 1310 - 13100 psi @Temperature 257 - 527 °F |
| Flexural Modulus | 2.12 - 24.0 GPa | 307 - 3480 ksi |
| 0.20312 - 0.20312 GPa @Temperature 204 - 204 °C | 29.460 - 29.460 ksi @Temperature 400 - 400 °F |
| Flexural Strain at Break | 3.00 - 7.00 % | 3.00 - 7.00 % |
| Compressive Yield Strength | 12.0 - 300 MPa | 1740 - 43500 psi |
| 65.0 - 80.0 MPa @Temperature 120 - 120 °C | 9430 - 11600 psi @Temperature 248 - 248 °F |
| Compressive Modulus | 2.48 - 4.25 GPa | 360 - 617 ksi |
| Shear Strength | 55.0 - 90.0 MPa | 7980 - 13100 psi |
| 14.3411 - 68.2581 MPa @Temperature 65.6 - 288 °C | 2080.00 - 9900.02 psi @Temperature 150 - 550 °F |
| Izod Impact, Notched | 0.310 - 11.4 J/cm | 0.580 - 21.4 ft-lb/in |
| Izod Impact, Unnotched | 13.3 - 25.6 J/cm | 25.0 - 48.0 ft-lb/in |
| Izod Impact, Notched (ISO) | 0.450 - 10.5 kJ/m² | 0.214 - 5.00 ft-lb/in² |
| Izod Impact, Unnotched (ISO) | 5.50 kJ/m² - NB | 2.62 ft-lb/in² - NB |
| Charpy Impact Unnotched | 2.50 J/cm² - NB | 11.9 ft-lb/in² - NB |
| 0.000 J/cm² - NB @Temperature -40.0 - -30.0 °C | 0.000 ft-lb/in² - NB @Temperature -40.0 - -22.0 °F |
| Charpy Impact, Notched | 0.100 - 8.00 J/cm² | 0.476 - 38.1 ft-lb/in² |
| 0.500 - 0.910 J/cm² @Temperature -40.0 - -30.0 °C | 2.38 - 4.33 ft-lb/in² @Temperature -40.0 - -22.0 °F |
| Coefficient of Friction | 0.150 - 0.400 | 0.150 - 0.400 |
| Coefficient of Friction, Static | 0.200 - 0.320 | 0.200 - 0.320 |
| K (wear) Factor | 2.00 - 403 x 10-8 mm³/N-M | 0.993 - 200 x 10-10 in³-min/ft-lb-hr |
| Limiting Pressure Velocity | 2.42 MPa-m/sec | 69000 psi-ft/min |
| |
| Electrical Properties | Metric | English | Comments |
|---|
| Electrical Resistivity | 15000 - 4.90e+16 ohm-cm | 15000 - 4.90e+16 ohm-cm |
| 1.00e+9 - 1.00e+15 ohm-cm @Temperature 125 - 275 °C | 1.00e+9 - 1.00e+15 ohm-cm @Temperature 257 - 527 °F |
| Surface Resistance | 3000 - 1.00e+18 ohm | 3000 - 1.00e+18 ohm |
| Insulation Resistance | 1.00e+12 ohm | 1.00e+12 ohm |
| Dielectric Constant | 2.20 - 10.9 | 2.20 - 10.9 |
| 4.50 - 4.50 @Temperature 200 - 200 °C | 4.50 - 4.50 @Temperature 392 - 392 °F |
| | 4.50 - 4.50 @Frequency 50.0 - 50.0 Hz | 4.50 - 4.50 @Frequency 50.0 - 50.0 Hz |
| Dielectric Strength | 15.7 - 200 kV/mm | 400 - 5080 kV/in |
| Dissipation Factor | 0.00100 - 0.518 | 0.00100 - 0.518 |
| Comparative Tracking Index | 125 - 200 V | 125 - 200 V |
| |
| Thermal Properties | Metric | English | Comments |
|---|
| CTE, linear | 4.70 - 216 µm/m-°C | 2.61 - 120 µin/in-°F |
| 10.8 - 252 µm/m-°C @Temperature 22.8 - 150 °C | 6.00 - 140 µin/in-°F @Temperature 73.0 - 302 °F |
| CTE, linear, Transverse to Flow | 47.0 - 252 µm/m-°C | 26.1 - 140 µin/in-°F |
| 140 - 160 µm/m-°C @Temperature >=143 °C | 77.8 - 88.9 µin/in-°F @Temperature >=289 °F |
| Specific Heat Capacity | 1.10 - 2.20 J/g-°C | 0.263 - 0.526 BTU/lb-°F |
| Thermal Conductivity | 0.173 - 0.950 W/m-K | 1.20 - 6.59 BTU-in/hr-ft²-°F |
| Melting Point | 178 - 386 °C | 352 - 726 °F |
| Maximum Service Temperature, Air | 150 - 310 °C | 302 - 590 °F |
| Deflection Temperature at 0.46 MPa (66 psi) | 152 - 336 °C | 306 - 637 °F |
| Deflection Temperature at 1.8 MPa (264 psi) | 140 - 336 °C | 284 - 637 °F |
| Vicat Softening Point | 280 - 335 °C | 536 - 635 °F |
| Softening Point | 168 °C | 334 °F |
| Minimum Service Temperature, Air | -100 - -20.0 °C | -148 - -4.00 °F |
| Glass Transition Temp, Tg | 143 - 180 °C | 289 - 356 °F |
| UL RTI, Electrical | 260 °C | 500 °F |
| UL RTI, Mechanical with Impact | 180 °C | 356 °F |
| UL RTI, Mechanical without Impact | 240 °C | 464 °F |
| Flammability, UL94 | V-1 - V-0 | V-1 - V-0 |
| Oxygen Index | 23.0 - 49.0 % | 23.0 - 49.0 % |
| Glow Wire Test | 800 - 960 °C | 1470 - 1760 °F |
| |
| Processing Properties | Metric | English | Comments |
|---|
| Processing Temperature | 100 - 410 °C | 212 - 770 °F |
| Nozzle Temperature | 360 - 440 °C | 680 - 824 °F |
| Melt Temperature | 174 - 470 °C | 345 - 878 °F |
| Mold Temperature | 149 - 250 °C | 300 - 482 °F |
| Injection Velocity | 200 mm/sec | 7.87 in/sec |
| Drying Temperature | 120 - 180 °C | 248 - 356 °F |
| Moisture Content | 0.0200 - 0.290 % | 0.0200 - 0.290 % |
| Injection Pressure | 82.7 - 124 MPa | 12000 - 18000 psi |
| Recrystallization Temperature | 285 °C | 545 °F |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.