MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Diphenyl ether, C12H10O
Categories: Fluid; Solvent

Key Words: C12H10O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.066 g/cc
@Temperature 20.0 °C
Viscosity 7.724 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 170.211 g/mol
Vapor Pressure 0.0100 torr
@Temperature 20.0 °C
Surface Tension 27.14 dynes/cm
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 31.0 atm
Critical Temperature 493 °C
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.87
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 276.8 J/g
Specific Heat Capacity 1.272 J/g-°C
 0.983 J/g-°C
@Temperature 25.0 °C
Vapor
Melting Point 26.9 °C
Boiling Point 258.1 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.576
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.3459
Antoine's Vapor Pressure B Parameter4310.25
Antoine's Vapor Pressure C Parameter-87.31
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)101-84-8
Chemical FormulaC12H10O
Critical Compressibility (Zc)0
Dipole moment (p/C.m)3.669E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A1146
Dynamic Viscosity Parameter B379.29
Henry's Law Constant (atm m3/mol)0.000118
Molar Heat Capacity (298K)167.327 J/mol-K
Molar Heat Capacity of Vapor a Parameter-60.6889
Molar Heat Capacity of Vapor b Parameter0.9276
Molar Heat Capacity of Vapor c Parameter-0.0006335
Molar Heat Capacity of Vapor d Parameter1.358E-07
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number3077

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2
2-Butanol (CH3CH2CH(OH)CH3; secondary-Butyl Alcohol)
1-Pentanol, C5H12O
1-Octanol, C8H18O

VORGS149 / 99525

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.