MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

1-Octanol, C8H18O
Categories: Fluid; Solvent

Key Words: C8H18O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.826 g/cc
@Temperature 20.0 °C
0.0298 lb/in³
@Temperature 68.0 °F
Viscosity 8.499 cP
@Temperature 20.0 °C
8.499 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 130.231 g/mol130.231 g/mol
Vapor Pressure 0.0000360 bar
@Temperature 20.0 °C
0.0270 torr
@Temperature 68.0 °F
Surface Tension 26.92 dynes/cm
@Temperature 20.0 °C
26.92 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 64.4 bar48300 torr
Critical Temperature -215 °C-355 °F
Critical Density 0.266 g/cc0.00961 lb/in³
Critical Molar Volume 490 cm³/mol29.9 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 10.34
@Temperature 20.0 °C
10.34
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 388.7 J/g167.2 BTU/lb
Specific Heat Capacity 2.346 J/g-°C0.5607 BTU/lb-°F
 1.542 J/g-°C
@Temperature 25.0 °C
0.3685 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.1614 W/m-K
@Temperature 20.0 °C
1.120 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -15.5 °C4.10 °F
Boiling Point 195.3 °C383.5 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.427
@Wavelength 589.3 nm
1.427
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter15.7428
Antoine's Vapor Pressure B Parameter3017.81
Antoine's Vapor Pressure C Parameter-137.1
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)111-87-5
Chemical FormulaC8H18O
Critical Compressibility (Zc)0.31
Dipole moment (p/C.m)6.671E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A1312.1
Dynamic Viscosity Parameter B369.97
Henry's Law Constant (atm m3/mol)2.52E-05
Molar Heat Capacity (298K)200.759 J/mol-K
Molar Heat Capacity of Vapor a Parameter6.1672
Molar Heat Capacity of Vapor b Parameter0.7602
Molar Heat Capacity of Vapor c Parameter-0.0003974
Molar Heat Capacity of Vapor d Parameter6.259E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF 2-Ethylhexanol
BASF 2-Ethylhexanal
3M Fluorinert™ FC-3283 Electronic Liquid
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2

VORGS274 / 99633

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.