MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

2-Butanol (CH3CH2CH(OH)CH3; secondary-Butyl Alcohol)
Categories: Fluid; Solvent

Key Words: OHCH3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.808 g/cc
@Temperature 20.0 °C
0.0292 lb/in³
@Temperature 68.0 °F
Viscosity  3.096 cP
@Temperature 25.0 °C
3.096 cP
@Temperature 77.0 °F
 3.706 cP
@Temperature 20.0 °C
3.706 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 74.12 g/mol74.12 g/mol
Vapor Pressure  0.040162 bar
@Temperature 20.0 °C
30.124 torr
@Temperature 68.0 °F
 0.1000 bar
@Temperature 48.2 °C
75.00 torr
@Temperature 119 °F
Surface Tension 23.47 dynes/cm
@Temperature 20.0 °C
23.47 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 42.02 bar31520 torr
Critical Temperature 263.08 °C505.54 °F
Critical Density 0.276 g/cc0.00997 lb/in³
Critical Molar Volume 269 cm³/mol16.4 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 17.26
@Temperature 20.0 °C
17.26
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 80.55 J/g34.65 BTU/lbEnthalpy of fusion at normal melting point
Heat of Vaporization 550.4 J/g236.8 BTU/lb
 670.8 J/g288.6 BTU/lbEnthalpy of vaporization at normal boiling temperature
Specific Heat Capacity 2.884 J/g-°C0.6893 BTU/lb-°F
 1.483 J/g-°C
@Temperature 25.0 °C
0.3544 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.1346 W/m-K
@Temperature 20.0 °C
0.9341 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -114.7 °C-174.5 °F
Boiling Point 99.51 °C
@Pressure 0.101 MPa
211.1 °F
@Pressure 14.7 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.3954
@Temperature 20.0 °C,
Wavelength 589.3 nm
1.3954
@Temperature 68.0 °F,
Wavelength 589.3 nm
Na D line
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.8548
Antoine's Vapor Pressure B Parameter2658.29
Antoine's Vapor Pressure C Parameter-95.5
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)78-92-2
Chemical FormulaC4H10O
Critical Compressibility (Zc)0.259
Dipole moment (p/C.m)5.671E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A972.1
Dynamic Viscosity Parameter B363.38
Henry's Law Constant (atm m3/mol)1.73E-05
Molar Heat Capacity (298K)109.912 J/mol-K
Molar Heat Capacity of Vapor a Parameter-48.5804
Molar Heat Capacity of Vapor b Parameter0.7167
Molar Heat Capacity of Vapor c Parameter-0.0007079
Molar Heat Capacity of Vapor d Parameter2.918E-07
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1120

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell Heptane
Honeywell Hexane
Honeywell Hexane Laboratory Plus
Honeywell Hexane Purified Plus®
3M Fluorinert™ FC-3283 Electronic Liquid

VORG005 / 74516

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.