MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

1-Pentanol, C5H12O
Categories: Fluid; Solvent

Key Words: C5H12O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.815 g/cc
@Temperature 20.0 °C
0.0294 lb/in³
@Temperature 68.0 °F
Viscosity 4.308 cP
@Temperature 20.0 °C
4.308 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 88.15 g/mol88.15 g/mol
Vapor Pressure 0.002069 bar
@Temperature 20.0 °C
1.552 torr
@Temperature 68.0 °F
Surface Tension 25.6 dynes/cm
@Temperature 20.0 °C
25.6 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 38.5 bar28900 torr
Critical Temperature 313 °C595 °F
Critical Density 0.270 g/cc0.00975 lb/in³
Critical Molar Volume 326 cm³/mol19.9 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 13.9
@Temperature 20.0 °C
13.9
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 503.1 J/g216.4 BTU/lb
Specific Heat Capacity 2.37 J/g-°C0.566 BTU/lb-°F
 1.499 J/g-°C
@Temperature 25.0 °C
0.3583 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.153 W/m-K
@Temperature 20.0 °C
1.06 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -78.2 °C-109 °F
Boiling Point 137.9 °C280.2 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.41
@Wavelength 589.3 nm
1.41
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.527
Antoine's Vapor Pressure B Parameter3026.89
Antoine's Vapor Pressure C Parameter-405
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)71-41-0
Chemical FormulaC5H12O
Critical Compressibility (Zc)0.26
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A1151.4
Dynamic Viscosity Parameter B349.62
Henry's Law Constant (atm m3/mol)1.3E-05
Molar Heat Capacity (298K)132.095 J/mol-K
Molar Heat Capacity of Vapor a Parameter3.866
Molar Heat Capacity of Vapor b Parameter0.5042
Molar Heat Capacity of Vapor c Parameter-0.0002638
Molar Heat Capacity of Vapor d Parameter5.117E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1105
UV cut-off (nm)210

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
1,4-Butanediol, C4H10O2
1,1,1 Trichloroethane (CH3CCl3)
2-Butoxyethanol, C6H14O2
2-Butanol (CH3CH2CH(OH)CH3; secondary-Butyl Alcohol)
1-Octanol, C8H18O

VORGS281 / 99639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.