MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

1,1,1 Trichloroethane (CH3CCl3)
Categories: Fluid; Solvent

Material Notes: Widely used as a solvent and as a cold cleaning and vapor degreasing agent. Previously used in household products, including sprays, spot removers, adhesives, and lubricants. It is being phased out of many uses due to environmental and health concerns.

Information provided by Enviro Tech International and the reference(s).

Key Words: CH3CCl3, a-trichloroethane, chloroethene, methylchloroform, methyltrichloromethane, TCEA, trichloromethylmethane
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.00555 g/cc0.000201 lb/in³Vapor Density
 1.32 g/cc
@Temperature 25.0 °C
0.0477 lb/in³
@Temperature 77.0 °F
 1.339 g/cc
@Temperature 20.0 °C
0.04837 lb/in³
@Temperature 68.0 °F
Viscosity 0.79 cP
@Temperature 25.0 °C
0.79 cP
@Temperature 77.0 °F
Molecular Weight 133.4 g/mol133.4 g/mol
Vapor Pressure 0.133 bar
@Temperature 20.0 °C
100 torr
@Temperature 68.0 °F
Surface Tension 25.6 dynes/cm25.6 dynes/cm200°C
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 7.252
@Temperature 20.0 °C
7.252
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 241 J/g104 BTU/lb
Specific Heat Capacity 1.05 J/g-°C0.250 BTU/lb-°F
Thermal Conductivity 0.1012 W/m-K
@Temperature 20.0 °C
0.7023 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -30.4 °C-22.7 °F
Boiling Point 74.0 °C165 °F
Decomposition Temperature 200 °C392 °F
Flammability Test 8.0 - 138.0 - 13vol% limits
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.437
@Wavelength 589.3 nm
1.437
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Atmospheric Lifetime5.4 years
CAS Number71-55-6
CAS registry number (CARN)71-55-6
Chemical FormulaC2H3Cl3
Evaporation Rate (n-Butyl Acetate = 1)4.55ASTM D-3539-76
Flash Point TCCNone
Hansen Parameter Non-Polar17
Hansen Parameter Polar5.8
Henry's Law Constant (atm m3/mol)0.003
Hildebrand Parameter17.4
Kauri Butanol Number124
Ozone Depletion Potential (ODP)> 0.10
UN Number2831

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
1-Pentanol, C5H12O
1,1,1,2-Tetrabromoethane (acetylene tetrabromide), C2H2Br4
18-18-2 Austenitic Stainless Steel, Annealed Plate, Sheet, Strip, UNS S38100
1,4-Butanediol, C4H10O2
17-7 PH Stainless Steel, CH900, plate, sheet, and strip

VORG043 / 74554

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.