MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC Ultem 1000FV PEI  (discontinued **)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.

This data was supplied by SABIC-IP for the Americas region.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D 792
Density 1.27 g/cc0.0459 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.70 %0.70 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.25 %
@Temperature 23.0 °C
1.25 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC Method
Melt Flow  9.0 g/10 min
@Load 6.60 kg,
Temperature 337 °C
9.0 g/10 min
@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
 13 g/10 min
@Load 5.00 kg,
Temperature 220 °C
13 g/10 min
@Load 11.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa12300 psi5 mm/min; ISO 527
 90.0 MPa13100 psiType I, 5 mm/min; ASTM D 638
Tensile Strength, Yield 105 MPa15200 psi5 mm/min; ISO 527
 110 MPa16000 psiType I, 5 mm/min; ASTM D 638
Elongation at Break 60 %60 %Type I, 5 mm/min; ASTM D 638
 60 %60 %5 mm/min; ISO 527
Elongation at Yield 6.0 %6.0 %5 mm/min; ISO 527
 7.0 %7.0 %Type I, 5 mm/min; ASTM D 638
Tensile Modulus 3.20 GPa464 ksi1 mm/min; ISO 527
 3.58 GPa519 ksi5 mm/min; ASTM D 638
Flexural Yield Strength 160 MPa23200 psi2 mm/min; ISO 178
 173 MPa25100 psi1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 3.30 GPa479 ksi2 mm/min; ISO 178
 3.43 GPa497 ksi1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched  0.530 J/cm
@Temperature 23.0 °C
0.993 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
 0.550 J/cm
@Temperature -30.0 °C
1.03 ft-lb/in
@Temperature -22.0 °F
ASTM D 256
Izod Impact, Unnotched 13.35 J/cm
@Temperature 23.0 °C
25.01 ft-lb/in
@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO)  6.00 kJ/m²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmASTM D 257
Dielectric Constant 3.15
@Frequency 1000 Hz
3.15
@Frequency 1000 Hz
ASTM D 150
Dielectric Strength  27.9 kV/mm
@Thickness 1.60 mm
709 kV/in
@Thickness 0.0630 in
in oil; ASTM D 149
 32.7 kV/mm
@Thickness 1.60 mm
831 kV/in
@Thickness 0.0630 in
in air; ASTM D 149
Dissipation Factor  0.0013
@Frequency 1000 Hz
0.0013
@Frequency 1000 Hz
ASTM D 150
 0.0025
@Frequency 2.45e+9 Hz
0.0025
@Frequency 2.45e+9 Hz
ASTM D 150
Arc Resistance 120 - 180 sec120 - 180 secTungsten, PLC code 5; ASTM D 495
Comparative Tracking Index 100 - 175 V100 - 175 VPLC code 4; UL 746A
Hot Wire Ignition, HWI 60 - 120 sec60 - 120 secPLC code 1; UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs15 - 30 arcssurface, PLC code 3; UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min1.00 - 3.15 in/minPLC code 2; UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  50.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
27.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 55.8 µm/m-°C
@Temperature -20.0 - 150 °C
31.0 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E 831
CTE, linear, Transverse to Flow  50.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
27.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 54.0 µm/m-°C
@Temperature -20.0 - 150 °C
30.0 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 201 °C
@Thickness 6.40 mm
394 °F
@Thickness 0.252 in
unannealed; ASTM D 648
Vicat Softening Point 211 °C412 °FRate B/120; ISO 306
 215 °C419 °FRate B/50; ISO 306
 218 °C424 °FRate B/50; ASTM D 1525
Glass Transition Temp, Tg 217 °C423 °F
UL RTI, Electrical 170 °C338 °FUL 746B
UL RTI, Mechanical with Impact 170 °C338 °FUL 746B
UL RTI, Mechanical without Impact 170 °C338 °FUL 746B
Flammability, UL94  V-2
@Thickness 0.400 mm
V-2
@Thickness 0.0157 in
UL 94
 V-1
@Thickness 0.750 mm
V-1
@Thickness 0.0295 in
UL 94
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
UL 94
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
UL 94
Smoke Density 0.70
@Time 240 sec
0.70
@Time 0.0667 hour
NBS, Flaming, Ds; ASTM E 662
Oxygen Index 47 %47 %LOI; ASTM D 2863
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo EMERGE™ PC 8701-15 Polycarbonate Resin
Teijin Multilon DN-3510F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polycarbonate, Molded
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded

PSABIC2897 / 116785

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.