MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Microtherm Group Molded Pipe Sections Filament Reinforced Silica Pipe Insulation
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material

Material Notes: Microtherm® Moulded Pipe Sections (MPS) are preformed pieces of pipe insulation designed to provide a thermally efficient insulation system for piping of all sizes from 25 mm (1”) upwards. Formulation based on pyrogenic silica with a mineral oxide opacifier and E-glass filament reinforcement.
    Properties
  • Microporous insulation offering the lowest theoretically possible thermal conductivity for continuous operation at temperatures up to to 1000 °C (1832 °F)
  • Precision molded pipe insulation sections
  • Can be applied in multi layer systems
  • Non combustible
  • Environmentally friendly
  • Free of harmful respirable fibers.
    Typical Applications
  • All pipeline applications
  • Round ducting applications
  • Passive fire protection to piping systems.

Information provided by Microtherm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 - 0.350 g/cc
Thickness 25000 microns
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 0.0420 MPaResistance at 10%, 350 kg/m³; ASTM C165
Compressive Modulus 4.40 MPa@ 350 kg/m³; ASTM C165
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.680 J/g-°C
@Temperature 0.000 °C
 0.920 J/g-°C
@Temperature 200 °C
 1.00 J/g-°C
@Temperature 400 °C
 1.04 J/g-°C
@Temperature 600 °C
 1.08 J/g-°C
@Temperature 800 °C
Thermal Conductivity 0.0221 W/m-K
@Temperature 100 °C
@ 320 kg/m³; ASTM C177, ISO 8302
 0.0222 W/m-K
@Temperature 200 °C
@ 320 kg/m³; ASTM C177, ISO 8302
 0.0230 W/m-K
@Temperature 300 °C
@ 320 kg/m³; ASTM C177, ISO 8302
 0.0244 W/m-K
@Temperature 400 °C
@ 320 kg/m³; ASTM C177, ISO 8302
 0.0260 W/m-K
@Temperature 500 °C
@ 320 kg/m³; ASTM C177, ISO 8302
 0.0281 W/m-K
@Temperature 600 °C
@ 320 kg/m³; ASTM C177, ISO 8302
 0.0343 W/m-K
@Temperature 800 °C
@ 320 kg/m³; ASTM C177, ISO 8302
Maximum Service Temperature, Air 1000 °Cfor long term exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alclad Aluminum 6061-T6, T651
Microtherm Group Freemoldings Pyrogenic Silica Thermal Insulation, E-Glass Reinforced
3M Nextel™ 720 Composite Ceramic Fiber
Tisan TISESTER® 30% Glass Fiber Reinforced, Impact Resistance and Heat Stabilized ISI Stab. Polybutylene Terephthalate
JIS SCM435 Chromium Molybdenum Steel

CMICRO11 / 90053

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.