MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tisan TISESTER® 30% Glass Fiber Reinforced, Impact Resistance and Heat Stabilized ISI Stab. Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Impact Grade

Material Notes: TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include:
  • Excellent surface appearance
  • High corrosion and abrasion resistance
  • Excellent toughness
  • High temperature resistance
  • Excellent chemical resistance
  • Electrical isolation and arc resistance
  • High performance
  • Easy processability
  • Fast cycle time
Glass fiber reinforcement imparts high shrinkage resistance and impact resistance to TISESTER products, yielding improvements in thermal features as well. PBT is resistant against solvents, exhibits low shrinkage during shaping, and it is mechanically strong, heat resistant for temperatures up to 150°C, and can be reinforced for flame retardance. Tisester compounds display sufficient resistance against hydrocarbons, alcohols, ethers, acids, and alkali solvents.

Key Words: PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ISO 1183
Moisture Absorption 0.20 %0.20 %ISO 62
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/in
Ash 30 %30 %ISO 3451
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psiISO 527-2
Tensile Strength, Yield 135 MPa19600 psiISO 527-2
Elongation at Break 4.0 %4.0 %ISO 527-2
Elongation at Yield 4.5 %4.5 %ISO 527-2
Modulus of Elasticity 8.00 GPa1160 ksiISO 527-2
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 400 V400 VTS EN 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 - 230 °C437 - 446 °F
Vicat Softening Point 210 °C410 °FISO 306
Heat Distortion Temperature 220 °C428 °FISO 75-2
Flammability, UL94 HBHB
Glow Wire Test 750 °C1380 °F60695-2-10
 
Processing PropertiesMetricEnglishComments
Feed Temperature 70.0 °C158 °F
Rear Barrel Temperature 220 - 250 °C428 - 482 °FAft-1. Region Temperature
Middle Barrel Temperature 220 - 250 °C428 - 482 °FMid-2. Region Temperature
Front Barrel Temperature 220 - 250 °C428 - 482 °FPre-3. Region Temperature
Nozzle Temperature 225 °C437 °F
Melt Temperature 220 - 230 °C428 - 446 °F
Drying Temperature 110 - 120 °C230 - 248 °FPredrying Temperature
Dry Time 4 - 5 hour4 - 5 hourPredrying Time
 
Descriptive Properties
Block Temperature80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
Microtherm Group Molded Pipe Sections Filament Reinforced Silica Pipe Insulation
Evonik Vestodur® X9408 High Impact PBT
Eurotec® Tecodur® PB70 GR30 NL100 IL PBT, 30% glass fiber reinforced, impact modified, natural
Esstech X-690-0000 1,9-Nonanediol Diacrylate, C15H24O4

PTIS056 / 79491

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.