MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Microtherm Group Freemoldings Pyrogenic Silica Thermal Insulation, E-Glass Reinforced
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material

Material Notes: Microtherm® Molded Products are Microtherm® high temperature thermal insulation sections molded in precision tooling for repeat accuracy of form and size, normally in large batches. Formulation based on pyrogenic silica with a mineral oxide opacifier and E-glass filament reinforcement.
    Properties
  • Microporous insulation offering the lowest theoretically possible thermal conductivity at high temperatures
  • Capable of continuous operation at temperatures up to 1000 °C (1832 °F)
  • Optimized design for customer product assembly
  • Non combustible
  • Environmentally safe.
  • Free of harmful respirable fibers.
    Applications
  • Large batch manufacture of complex shapes.

Information provided by Microtherm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.400 g/cc0.0145 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 0.0420 MPa6.09 psiResistance at 10%, 350 kg/m³; ASTM C165
Compressive Modulus 0.00440 GPa0.638 ksi@ 350 kg/m³; ASTM C165
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  0.680 J/g-°C
@Temperature 0.000 °C
0.163 BTU/lb-°F
@Temperature 32.0 °F
 0.920 J/g-°C
@Temperature 200 °C
0.220 BTU/lb-°F
@Temperature 392 °F
 1.00 J/g-°C
@Temperature 400 °C
0.239 BTU/lb-°F
@Temperature 752 °F
 1.04 J/g-°C
@Temperature 600 °C
0.249 BTU/lb-°F
@Temperature 1110 °F
 1.08 J/g-°C
@Temperature 800 °C
0.258 BTU/lb-°F
@Temperature 1470 °F
Thermal Conductivity  0.0221 W/m-K
@Temperature 100 °C
0.153 BTU-in/hr-ft²-°F
@Temperature 212 °F
@ 320 kg/m³; ASTM C177, ISO 8302
 0.0222 W/m-K
@Temperature 200 °C
0.154 BTU-in/hr-ft²-°F
@Temperature 392 °F
@ 320 kg/m³; ASTM C177, ISO 8302
 0.0230 W/m-K
@Temperature 300 °C
0.160 BTU-in/hr-ft²-°F
@Temperature 572 °F
@ 320 kg/m³; ASTM C177, ISO 8302
 0.0244 W/m-K
@Temperature 400 °C
0.169 BTU-in/hr-ft²-°F
@Temperature 752 °F
@ 320 kg/m³; ASTM C177, ISO 8302
 0.0260 W/m-K
@Temperature 500 °C
0.180 BTU-in/hr-ft²-°F
@Temperature 932 °F
@ 320 kg/m³; ASTM C177, ISO 8302
 0.0281 W/m-K
@Temperature 600 °C
0.195 BTU-in/hr-ft²-°F
@Temperature 1110 °F
@ 320 kg/m³; ASTM C177, ISO 8302
 0.0343 W/m-K
@Temperature 800 °C
0.238 BTU-in/hr-ft²-°F
@Temperature 1470 °F
@ 320 kg/m³; ASTM C177, ISO 8302
Maximum Service Temperature, Air 1000 °C1830 °Ffor long term exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Microtherm Group Molded Pipe Sections Filament Reinforced Silica Pipe Insulation
DuPont MOLYKOTE® PG-75 GREASE
DuPont MOLYKOTE® 7325 GREASE
DuPont MOLYKOTE® 41 HIGH TEMPERATURE BEARING GREASE
DuPont MOLYKOTE® 1122 CHAIN AND OPEN GEAR GREASE

CMICRO07 / 90049

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.