MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont MOLYKOTE® 1122 CHAIN AND OPEN GEAR GREASE
Categories: Fluid; Lubricant

Material Notes: Former Dow Corning product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc
@Temperature 25.0 °C
0.950 g/cc
@Temperature 77.0 °F
Kinematic Viscosity 1500 cSt1500 cSt
Saybolt Viscosity at 100°F 255 SUS255 SUSBase Oil Viscosity
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 265.04 kg584.41 lb (mass)
Penetration P(0), 1/10 mm 250 - 280250 - 280
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 160 °C320 °F
Minimum Service Temperature, Air 10.0 °C50.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 60.0 Month60.0 Month
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy/Carbon Fiber Composite
Overview of materials for AISI 8000 Series Steel
Microtherm Group Freemoldings Pyrogenic Silica Thermal Insulation, E-Glass Reinforced
Indium Corp. Indalloy® 262 Tin-Copper Solder Alloy
Hexcel® HexTow® AS4 12K Standard Modulus Carbon Fiber (12,000 Filaments)

PDOWCO250 / 105951

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.