MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

JIS SCM435 Chromium Molybdenum Steel
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Low Alloy Steel

Material Notes: Forging temp.: 1205°C (2200°F) max. Annealing temp.: 790 - 845°C. Hardening temp.: 845 - 870°C.

Key Words: JIS G4105(79) SCM435, SCM 435, SCM-435; Comparable to AISI 4135, UNS G41350
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³(AISI 4135)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 187 - 229187 - 229annealed and cold drawn (AISI 4135)
Modulus of Elasticity 205 GPa29700 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical for steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000223 ohm-cm0.0000223 ohm-cm(AISI 4135)
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.477 J/g-°C0.114 BTU/lb-°F(AISI 4135)
Thermal Conductivity 42.7 W/m-K296 BTU-in/hr-ft²-°F(AISI 4135)
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.33 - 0.38 %0.33 - 0.38 %
Chromium, Cr 0.90 - 1.2 %0.90 - 1.2 %
Copper, Cu <= 0.30 %<= 0.30 %
Iron, Fe 97.33 - 97.87 %97.33 - 97.87 %As remainder
Manganese, Mn 0.60 - 0.85 %0.60 - 0.85 %
Molybdenum, Mo 0.15 - 0.30 %0.15 - 0.30 %
Nickel, Ni <= 0.25 %<= 0.25 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.15 - 0.35 %0.15 - 0.35 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 4135 Steel
JIS S45C Steel, Normalized
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
JIS S45C Steel, Tempered
34MoCr4 Alloy Steel

M9ZJSCM435 / 231107

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.