MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

n-Propyl acetate, C5H10O2
Categories: Fluid; Solvent

Key Words: C5H10O2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.887 g/cc
@Temperature 20.0 °C
0.0320 lb/in³
@Temperature 68.0 °F
Viscosity 0.571 cP
@Temperature 20.0 °C
0.571 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 102.134 g/mol102.134 g/mol
Vapor Pressure 0.033167 bar
@Temperature 20.0 °C
24.877 torr
@Temperature 68.0 °F
Surface Tension 24.28 dynes/cm
@Temperature 20.0 °C
24.28 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 33.3 bar25000 torr
Critical Temperature 276 °C529 °F
Critical Density 0.296 g/cc0.0107 lb/in³
Critical Molar Volume 345 cm³/mol21.1 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 6.002
@Temperature 20.0 °C
6.002
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 334.7 J/g144.0 BTU/lb
Specific Heat Capacity 1.921 J/g-°C0.4591 BTU/lb-°F
 1.313 J/g-°C
@Temperature 25.0 °C
0.3138 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.1431 W/m-K
@Temperature 20.0 °C
0.9931 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -95.2 °C-139 °F
Boiling Point 101.7 °C215.1 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.383
@Wavelength 589.3 nm
1.383
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.2291
Antoine's Vapor Pressure B Parameter2980.47
Antoine's Vapor Pressure C Parameter-64.15
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)109-60-4
Chemical FormulaC5H10O2
Critical Compressibility (Zc)0.252
Dipole moment (p/C.m)6.004E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A489.53
Dynamic Viscosity Parameter B255.83
Henry's Law Constant (atm m3/mol)0.000218
Molar Heat Capacity (298K)134.153 J/mol-K
Molar Heat Capacity of Vapor a Parameter15.4097
Molar Heat Capacity of Vapor b Parameter0.4498
Molar Heat Capacity of Vapor c Parameter-0.0001685
Molar Heat Capacity of Vapor d Parameter-1.438E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1276

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2
2-Butanol (CH3CH2CH(OH)CH3; secondary-Butyl Alcohol)
1-Pentanol, C5H12O
1-Octanol, C8H18O

VORGS306 / 99663

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.