MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAKEEP® 2000GF30 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: VESTAKEEP 2000 GF30 is a medium-viscosity, glass fiber-reinforced (30%) polyether ether ketone for injection molding. The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP 2000 GF30 are self-extinguishing. VESTAKEEP 2000 GF30 can be processed by common injection-molding machines for thermoplastics.

Information provided by Evonik

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/indetermined on 2 mm sheets with film gate at rim mold temperature 180°C; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/indetermined on 2 mm sheets with film gate at rim mold temperature 180°C; ISO 294-4
Melt Flow 17 g/10 min
@Load 5.00 kg,
Temperature 380 °C
17 g/10 min
@Load 11.0 lb,
Temperature 716 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 165 MPa23900 psiISO 527-1
Elongation at Break 2.0 %2.0 %ISO 527-1
Tensile Modulus 11.0 GPa1600 ksiISO 527-1
Charpy Impact Unnotched  5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 6.50 J/cm²
@Temperature -30.0 °C
30.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant  3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
IEC 60250
 3.4
@Frequency 50 Hz
3.4
@Frequency 50 Hz
IEC 60250
Dielectric Strength 16.0 kV/mm406 kV/inIEC 60243-1
Comparative Tracking Index 175 V175 V100 drops value; IEC 60112
 200 V200 VCTI; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
16.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359
Melting Point 340 °C644 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 338 °C640 °FISO 75-1
Deflection Temperature at 1.8 MPa (264 psi) 323 °C613 °FISO 75-1
Vicat Softening Point  335 °C
@Load 5.10 kg
635 °F
@Load 11.2 lb
Method B; ISO 306
 340 °C
@Load 1.02 kg
644 °F
@Load 2.25 lb
Method A; ISO 306
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
IEC60695
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
IEC60695
Glow Wire Ignition Temperature 825 °C
@Thickness 2.00 mm
1520 °F
@Thickness 0.0787 in
IEC 60695-2
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 380 - 400 °C716 - 752 °F
Mold Temperature 160 - 200 °C320 - 392 °F
 180 °C356 °FPreferred

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTAKEEP® 4000CF30 PEEK
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI
Evonik VESTAKEEP® 4000GF30 PEEK
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK)

PEVONIL209 / 196413

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.