MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAKEEP® 2000GF30 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: VESTAKEEP 2000 GF30 is a medium-viscosity, glass fiber-reinforced (30%) polyether ether ketone for injection molding. The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP 2000 GF30 are self-extinguishing. VESTAKEEP 2000 GF30 can be processed by common injection-molding machines for thermoplastics.

Information provided by Evonik

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cmdetermined on 2 mm sheets with film gate at rim mold temperature 180°C; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cmdetermined on 2 mm sheets with film gate at rim mold temperature 180°C; ISO 294-4
Melt Flow 17 g/10 min
@Load 5.00 kg,
Temperature 380 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 165 MPaISO 527-1
Elongation at Break 2.0 %ISO 527-1
Tensile Modulus 11000 MPaISO 527-1
Charpy Impact Unnotched 55.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 65.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 3.3
@Frequency 1e+6 Hz
IEC 60250
 3.4
@Frequency 50 Hz
IEC 60250
Dielectric Strength 16.0 kV/mmIEC 60243-1
Comparative Tracking Index 175 V100 drops value; IEC 60112
 200 VCTI; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359
Melting Point 340 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 338 °CISO 75-1
Deflection Temperature at 1.8 MPa (264 psi) 323 °CISO 75-1
Vicat Softening Point 335 °C
@Load 5.10 kg
Method B; ISO 306
 340 °C
@Load 1.02 kg
Method A; ISO 306
Flammability, UL94 V-0
@Thickness 1.60 mm
IEC60695
 V-0
@Thickness 3.20 mm
IEC60695
Glow Wire Ignition Temperature 825 °C
@Thickness 2.00 mm
IEC 60695-2
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
IEC 60695-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 - 400 °C
Mold Temperature 160 - 200 °C
 180 °CPreferred

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAKEEP® 4000CF30 PEEK
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI
Evonik VESTAKEEP® 4000GF30 PEEK
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK)

PEVONIL209 / 196413

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.