MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³
Linear Mold Shrinkage, Flow 0.0025 - 0.0050 cm/cm0.0025 - 0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0060 - 0.0090 cm/cm0.0060 - 0.0090 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  110 MPa
@Temperature 150 °C
16000 psi
@Temperature 302 °F
 135 MPa
@Temperature 120 °C
19600 psi
@Temperature 248 °F
 155 MPa
@Temperature 90.0 °C
22500 psi
@Temperature 194 °F
 160 MPa
@Temperature 60.0 °C
23200 psi
@Temperature 140 °F
 175 MPa
@Temperature 23.0 °C
25400 psi
@Temperature 73.4 °F
Elongation at Break  2.2 %
@Temperature 23.0 °C
2.2 %
@Temperature 73.4 °F
 2.2 %
@Temperature 60.0 °C
2.2 %
@Temperature 140 °F
 2.2 %
@Temperature 90.0 °C
2.2 %
@Temperature 194 °F
 2.4 %
@Temperature 150 °C
2.4 %
@Temperature 302 °F
 23 %
@Temperature 120 °C
23 %
@Temperature 248 °F
Tensile Modulus  10.4 GPa
@Temperature 150 °C
1510 ksi
@Temperature 302 °F
 10.6 GPa
@Temperature 120 °C
1540 ksi
@Temperature 248 °F
 11.0 GPa
@Temperature 90.0 °C
1600 ksi
@Temperature 194 °F
 11.3 GPa
@Temperature 60.0 °C
1640 ksi
@Temperature 140 °F
 11.5 GPa
@Temperature 23.0 °C
1670 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 7.00 J/cm²33.3 ft-lb/in²
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 230 °C446 °F
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C>= 572 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 300 °C>= 572 °F
Vicat Softening Point >= 300 °C
@Load 5.00 kg
>= 572 °F
@Load 11.0 lb
Flammability, UL94  V-1
@Thickness 0.750 mm
V-1
@Thickness 0.0295 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Glow Wire Test 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
Glow Wire Ignition Temperature 875 °C
@Thickness 1.00 mm
1610 °F
@Thickness 0.0394 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 370 - 400 °C698 - 752 °F
Mold Temperature 170 - 200 °C338 - 392 °F
Drying Temperature 120 - 150 °C
@Time 10800 sec
248 - 302 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI
Evonik VESTAKEEP® 2000GF30 PEEK
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced
Oxford Polymers 30GF 30% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding

PLATH9646 / 177342

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.