MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance.
  • Excellent flexural, impact, and tensile characteristics
  • Very high continuous working temp
  • Very high heat distortion temp
  • Exceptional chemical resistance
  • Superior dielectric at high temperatures and frequencies
  • Good radiation resistance
  • Outstanding wear and abrasion resistance
  • Low smoke and toxic gas emissions
  • Excellent hydrolysis resistance

Information Provided by Ensinger Inc.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ASTM D792
Water Absorption 0.11 %0.11 %at 24 hours; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 103103ASTM D785
Tensile Strength, Yield 157 MPa22800 psiASTM D638
Elongation at Break 2.2 %2.2 %ASTM D638
Tensile Modulus 9.6995 GPa1406.8 ksi1 % Sec; ASTM D638
Flexural Strength 233 MPa33800 psiASTM D790
Flexural Modulus 10.309 GPa1495.2 ksiTangent; ASTM D790
Compressive Strength 215 MPa31200 psiASTM D695
Shear Strength 97.2 MPa14100 psiUltimate; ASTM D3846
Izod Impact, Notched 0.961 J/cm1.80 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistivity per Square 1.00e+16 ohm1.00e+16 ohmASTM D257
Dielectric Strength 6.89 kV/mm175 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.6 µm/m-°C
@Temperature 20.0 °C
12.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.432 W/m-K3.00 BTU-in/hr-ft²-°FASTM C177
Melting Point 334 °C633 °F
Maximum Service Temperature, Air 250 °C482 °FContinuous
Deflection Temperature at 1.8 MPa (264 psi) 316 °C600 °FASTM D648
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK)
Overview of materials for Polyetheretherketone, Unreinforced
G-11 Fiberglass Epoxy Laminate Sheet
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI

PENS27 / 35981

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.