MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66, 20% Mineral Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Mineral Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.54 g/cc0.0434 - 0.0556 lb/in³Average value: 1.27 g/cc Grade Count:29
 1.08 - 1.08 g/cc
@Temperature >=263 °C
0.0390 - 0.0390 lb/in³
@Temperature >=505 °F
Average value: 1.08 g/cc Grade Count:1
Filler Content 18.0 - 20.0 %18.0 - 20.0 %Average value: 19.6 % Grade Count:5
Water Absorption 0.500 - 7.70 %0.500 - 7.70 %Average value: 2.13 % Grade Count:11
Moisture Absorption at Equilibrium 2.00 - 2.50 %2.00 - 2.50 %Average value: 2.17 % Grade Count:6
Maximum Moisture Content 0.0900 - 0.1500.0900 - 0.150Average value: 0.113 Grade Count:3
Linear Mold Shrinkage 0.00200 - 0.0250 cm/cm0.00200 - 0.0250 in/inAverage value: 0.0114 cm/cm Grade Count:26
Linear Mold Shrinkage, Transverse 0.00600 - 0.0170 cm/cm0.00600 - 0.0170 in/inAverage value: 0.0124 cm/cm Grade Count:7
Melt Flow 3.00 - 40.0 g/10 min3.00 - 40.0 g/10 minAverage value: 17.8 g/10 min Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115 - 122115 - 122Average value: 119 Grade Count:6
Tensile Strength, Ultimate 50.0 - 120 MPa7250 - 17400 psiAverage value: 72.9 MPa Grade Count:23
 40.0 - 100 MPa
@Temperature -40.0 - 80.0 °C
5800 - 14500 psi
@Temperature -40.0 - 176 °F
Average value: 71.0 MPa Grade Count:1
Tensile Strength, Yield 70.0 - 95.0 MPa10200 - 13800 psiAverage value: 83.1 MPa Grade Count:6
Elongation at Break 1.00 - 50.0 %1.00 - 50.0 %Average value: 9.56 % Grade Count:25
Modulus of Elasticity 1.80 - 6.60 GPa261 - 957 ksiAverage value: 4.09 GPa Grade Count:14
Flexural Yield Strength 78.0 - 245 MPa11300 - 35500 psiAverage value: 125 MPa Grade Count:24
 57.0 - 160 MPa
@Temperature -40.0 - 80.0 °C
8270 - 23200 psi
@Temperature -40.0 - 176 °F
Average value: 113 MPa Grade Count:1
Flexural Modulus 2.50 - 9.00 GPa363 - 1310 ksiAverage value: 4.17 GPa Grade Count:23
 1.60 - 6.40 GPa
@Temperature -40.0 - 80.0 °C
232 - 928 ksi
@Temperature -40.0 - 176 °F
Average value: 4.28 GPa Grade Count:1
Izod Impact, Notched 0.200 - 1.55 J/cm0.375 - 2.90 ft-lb/inAverage value: 0.539 J/cm Grade Count:13
 0.350 - 0.450 J/cm
@Temperature -40.0 - -40.0 °C
0.656 - 0.843 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 0.400 J/cm Grade Count:1
Izod Impact, Notched (ISO) 6.00 - 95.0 kJ/m²2.86 - 45.2 ft-lb/in²Average value: 25.1 kJ/m² Grade Count:5
 8.00 - 8.00 kJ/m²
@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 8.00 kJ/m² Grade Count:1
Charpy Impact Unnotched 3.70 J/cm² - NB17.6 ft-lb/in² - NBAverage value: 6.18 J/cm² Grade Count:8
 1.00 - 10.0 J/cm²
@Temperature -20.0 - -20.0 °C
4.76 - 47.6 ft-lb/in²
@Temperature -4.00 - -4.00 °F
Average value: 5.10 J/cm² Grade Count:3
Charpy Impact, Notched 0.300 - 1.50 J/cm²1.43 - 7.14 ft-lb/in²Average value: 0.914 J/cm² Grade Count:12
 0.100 - 1.20 J/cm²
@Temperature -30.0 - -20.0 °C
0.476 - 5.71 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 0.479 J/cm² Grade Count:6
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+10 - 1.00e+15 ohm-cm1.00e+10 - 1.00e+15 ohm-cmAverage value: 4.19e+14 ohm-cm Grade Count:15
Surface Resistance 1.00e+10 - 1.00e+15 ohm1.00e+10 - 1.00e+15 ohmAverage value: 1.60e+14 ohm Grade Count:7
Dielectric Constant 3.70 - 6.003.70 - 6.00Average value: 4.38 Grade Count:4
Dielectric Strength 16.0 - 90.0 kV/mm406 - 2290 kV/inAverage value: 40.0 kV/mm Grade Count:9
Comparative Tracking Index 450 - 600 V450 - 600 VAverage value: 546 V Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 52.2 - 100 µm/m-°C29.0 - 55.6 µin/in-°FAverage value: 70.1 µm/m-°C Grade Count:4
Specific Heat Capacity 2.32 - 2.32 J/g-°C
@Temperature >=263 °C
0.554 - 0.554 BTU/lb-°F
@Temperature >=505 °F
Average value: 2.32 J/g-°C Grade Count:1
Thermal Conductivity 0.190 - 0.190 W/m-K
@Temperature >=263 °C
1.32 - 1.32 BTU-in/hr-ft²-°F
@Temperature >=505 °F
Average value: 0.190 W/m-K Grade Count:1
Melting Point 255 - 265 °C491 - 509 °FAverage value: 259 °C Grade Count:13
Maximum Service Temperature, Air 80.0 - 220 °C176 - 428 °FAverage value: 140 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 140 - 250 °C284 - 482 °FAverage value: 218 °C Grade Count:17
Deflection Temperature at 1.8 MPa (264 psi) 75.0 - 230 °C167 - 446 °FAverage value: 132 °C Grade Count:23
Vicat Softening Point 155 - 260 °C311 - 500 °FAverage value: 220 °C Grade Count:6
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:19
Glow Wire Test 650 °C1200 °FAverage value: 650 °C Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 310 °C518 - 590 °FAverage value: 293 °C Grade Count:4
Melt Temperature 250 - 310 °C482 - 590 °FAverage value: 284 °C Grade Count:16
Mold Temperature 49.0 - 120 °C120 - 248 °FAverage value: 85.9 °C Grade Count:19
Drying Temperature 71.0 - 110 °C160 - 230 °FAverage value: 86.7 °C Grade Count:15
Moisture Content 0.100 - 0.200 %0.100 - 0.200 %Average value: 0.175 % Grade Count:6
Injection Pressure 30.0 - 124 MPa4350 - 18000 psiAverage value: 83.6 MPa Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 10% Mineral Filled
Overview of materials for Nylon 66, 30% Mineral Filled
Overview of materials for Nylon 66, 40% Glass Fiber Filled
Overview of materials for Nylon 66, 40% Mineral Filled
Aluminum 2011-T6

O2532 / 78029

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.