MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66, 30% Mineral Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Mineral Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 - 1.62 g/cc0.0470 - 0.0585 lb/in³Average value: 1.39 g/cc Grade Count:46
 1.40 - 1.40 g/cc
@Temperature 290 - 290 °C
0.0506 - 0.0506 lb/in³
@Temperature 554 - 554 °F
Average value: 1.40 g/cc Grade Count:1
Filler Content 25.0 - 32.0 %25.0 - 32.0 %Average value: 29.5 % Grade Count:6
Water Absorption 0.400 - 6.20 %0.400 - 6.20 %Average value: 1.80 % Grade Count:22
Moisture Absorption at Equilibrium 0.170 - 2.30 %0.170 - 2.30 %Average value: 1.49 % Grade Count:10
Water Absorption at Saturation 5.00 - 8.00 %5.00 - 8.00 %Average value: 5.80 % Grade Count:5
Maximum Moisture Content 0.0900 - 0.1500.0900 - 0.150Average value: 0.110 Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cm0.00100 - 0.0200 in/inAverage value: 0.0100 cm/cm Grade Count:43
Linear Mold Shrinkage, Transverse 0.00600 - 0.0200 cm/cm0.00600 - 0.0200 in/inAverage value: 0.0117 cm/cm Grade Count:18
Melt Flow 1.00 - 20.0 g/10 min1.00 - 20.0 g/10 minAverage value: 7.33 g/10 min Grade Count:6
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 90.090.0Average value: 90.0 Grade Count:3
Hardness, Rockwell R 115 - 125115 - 125Average value: 120 Grade Count:14
Tensile Strength, Ultimate 40.0 - 159 MPa5800 - 23000 psiAverage value: 74.6 MPa Grade Count:34
Tensile Strength, Yield 73.5 - 186 MPa10700 - 27000 psiAverage value: 98.9 MPa Grade Count:13
Elongation at Break 1.00 - 50.0 %1.00 - 50.0 %Average value: 8.66 % Grade Count:38
Elongation at Yield 3.00 - 16.0 %3.00 - 16.0 %Average value: 8.33 % Grade Count:3
Modulus of Elasticity 1.90 - 9.31 GPa276 - 1350 ksiAverage value: 5.06 GPa Grade Count:22
Flexural Yield Strength 50.0 - 241 MPa7250 - 35000 psiAverage value: 128 MPa Grade Count:31
Flexural Modulus 1.80 - 9.65 GPa261 - 1400 ksiAverage value: 4.73 GPa Grade Count:38
Poissons Ratio 0.350 - 0.4100.350 - 0.410Average value: 0.369 Grade Count:4
Izod Impact, Notched 0.196 - 1.10 J/cm0.367 - 2.06 ft-lb/inAverage value: 0.531 J/cm Grade Count:22
Izod Impact, Unnotched 2.67 - 14.9 J/cm5.00 - 28.0 ft-lb/inAverage value: 8.19 J/cm Grade Count:3
Izod Impact, Notched (ISO) 2.00 - 330 kJ/m²0.952 - 157 ft-lb/in²Average value: 36.0 kJ/m² Grade Count:12
 1.90 - 100 kJ/m²
@Temperature -40.0 - -30.0 °C
0.904 - 47.6 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 23.7 kJ/m² Grade Count:5
Izod Impact, Unnotched (ISO) 9.00 - 330 kJ/m²4.28 - 157 ft-lb/in²Average value: 105 kJ/m² Grade Count:4
 5.00 - 85.0 kJ/m²
@Temperature -40.0 - -30.0 °C
2.38 - 40.4 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 34.6 kJ/m² Grade Count:3
Charpy Impact Unnotched 1.80 J/cm² - NB8.57 ft-lb/in² - NBAverage value: 8.38 J/cm² Grade Count:20
 1.10 - 12.0 J/cm²
@Temperature -40.0 - -20.0 °C
5.24 - 57.1 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 4.57 J/cm² Grade Count:14
Charpy Impact, Notched 0.200 - 1.50 J/cm²0.952 - 7.14 ft-lb/in²Average value: 0.585 J/cm² Grade Count:18
 0.150 - 1.00 J/cm²
@Temperature -40.0 - -20.0 °C
0.714 - 4.76 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.433 J/cm² Grade Count:12
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+11 - 1.00e+17 ohm-cm1.00e+11 - 1.00e+17 ohm-cmAverage value: 9.16e+15 ohm-cm Grade Count:21
Surface Resistance 1.00e+10 - 1.00e+15 ohm1.00e+10 - 1.00e+15 ohmAverage value: 9.68e+13 ohm Grade Count:11
Dielectric Constant 3.40 - 9.103.40 - 9.10Average value: 4.40 Grade Count:9
Dielectric Strength 15.0 - 85.0 kV/mm380 - 2160 kV/inAverage value: 34.2 kV/mm Grade Count:21
Dissipation Factor 0.0100 - 0.05000.0100 - 0.0500Average value: 0.0219 Grade Count:4
Comparative Tracking Index 300 - 600 V300 - 600 VAverage value: 471 V Grade Count:13
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.8 - 65.0 µm/m-°C11.0 - 36.1 µin/in-°FAverage value: 49.0 µm/m-°C Grade Count:14
CTE, linear, Transverse to Flow 65.0 - 81.0 µm/m-°C36.1 - 45.0 µin/in-°FAverage value: 75.3 µm/m-°C Grade Count:3
Specific Heat Capacity 1.70 - 1.70 J/g-°C
@Temperature 290 - 290 °C
0.406 - 0.406 BTU/lb-°F
@Temperature 554 - 554 °F
Average value: 1.70 J/g-°C Grade Count:1
Thermal Conductivity 0.230 - 0.230 W/m-K
@Temperature 290 - 290 °C
1.60 - 1.60 BTU-in/hr-ft²-°F
@Temperature 554 - 554 °F
Average value: 0.230 W/m-K Grade Count:1
Melting Point 254 - 265 °C490 - 509 °FAverage value: 259 °C Grade Count:31
Maximum Service Temperature, Air 80.0 - 220 °C176 - 428 °FAverage value: 130 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 145 - 260 °C293 - 500 °FAverage value: 224 °C Grade Count:25
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 256 °C140 - 492 °FAverage value: 147 °C Grade Count:41
Vicat Softening Point 200 - 265 °C392 - 509 °FAverage value: 236 °C Grade Count:17
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:30
Flame Spread 0.000 - 80.0 mm/min0.000 - 3.15 in/minAverage value: 53.3 mm/min Grade Count:3
Oxygen Index 24.0 - 40.0 %24.0 - 40.0 %Average value: 28.6 % Grade Count:8
Glow Wire Test 649 - 960 °C1200 - 1760 °FAverage value: 772 °C Grade Count:14
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 250 - 295 °C482 - 563 °FAverage value: 279 °C Grade Count:4
Melt Temperature 250 - 310 °C482 - 590 °FAverage value: 283 °C Grade Count:27
Mold Temperature 50.0 - 120 °C122 - 248 °FAverage value: 90.1 °C Grade Count:26
Drying Temperature 79.4 - 100 °C175 - 212 °FAverage value: 85.2 °C Grade Count:22
Moisture Content 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.167 % Grade Count:11
Injection Pressure 34.5 - 138 MPa5000 - 20000 psiAverage value: 95.2 MPa Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 10% Mineral Filled
Overview of materials for Nylon 66, 20% Mineral Filled
Overview of materials for Nylon 66, 40% Mineral Filled
BASF Ultramid® A3HG5 25% Glass Filled PA66 (Dry)
BASF Ultramid® A3HG5 25% Glass Filled PA66 (Conditioned)

O2533 / 78030

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.