MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66, 40% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.90 g/cc0.0434 - 0.0686 lb/in³Average value: 1.44 g/cc Grade Count:526
 1.24 - 1.29 g/cc
@Temperature 261 - 295 °C
0.0448 - 0.0466 lb/in³
@Temperature 502 - 563 °F
Average value: 1.25 g/cc Grade Count:9
Filler Content 30.0 - 43.0 %30.0 - 43.0 %Average value: 39.1 % Grade Count:81
Water Absorption 0.300 - 6.50 %0.300 - 6.50 %Average value: 1.88 % Grade Count:220
Moisture Absorption at Equilibrium 0.170 - 2.30 %0.170 - 2.30 %Average value: 1.50 % Grade Count:144
 1.30 - 2.00 %
@Temperature 70.0 - 70.0 °C
1.30 - 2.00 %
@Temperature 158 - 158 °F
Average value: 1.69 % Grade Count:21
Water Absorption at Saturation 3.50 - 8.00 %3.50 - 8.00 %Average value: 4.84 % Grade Count:85
Additive Loading 35.0 - 40.0 %35.0 - 40.0 %Average value: 39.0 % Grade Count:5
Viscosity 2.70 - 50.0 cP2.70 - 50.0 cPAverage value: 14.6 cP Grade Count:4
 238 - 238 cP
@Temperature 285 - 285 °C
238 - 238 cP
@Temperature 545 - 545 °F
Average value: 15900 cP Grade Count:1
 20.0 - 170000 cP
@Temperature 100 - 2000 °C
20.0 - 170000 cP
@Temperature 212 - 3630 °F
Average value: 15900 cP Grade Count:6
 20.0 - 170000 cP
@Shear Rate 10.0 - 10000 1/s
20.0 - 170000 cP
@Shear Rate 10.0 - 10000 1/s
Average value: 15900 cP Grade Count:6
Viscosity Test 140 - 150 cm³/g1.40 - 1.50 dl/gAverage value: 147 cm³/g Grade Count:3
Viscosity Number 110 - 146 cm³/g1.10 - 1.46 dl/gAverage value: 137 cm³/g Grade Count:18
Maximum Moisture Content 0.0200 - 0.2000.0200 - 0.200Average value: 0.168 Grade Count:20
Linear Mold Shrinkage 0.000300 - 0.0250 cm/cm0.000300 - 0.0250 in/inAverage value: 0.00405 cm/cm Grade Count:353
 0.00400 - 0.00400 cm/cm
@Temperature 80.0 - 80.0 °C
0.00400 - 0.00400 in/in
@Temperature 176 - 176 °F
Average value: 0.00400 cm/cm Grade Count:6
Linear Mold Shrinkage, Transverse 0.000900 - 0.0180 cm/cm0.000900 - 0.0180 in/inAverage value: 0.00796 cm/cm Grade Count:189
 0.00700 - 0.00700 cm/cm
@Temperature 80.0 - 80.0 °C
0.00700 - 0.00700 in/in
@Temperature 176 - 176 °F
Average value: 0.00700 cm/cm Grade Count:6
Melt Flow 1.00 - 56.4 g/10 min1.00 - 56.4 g/10 minAverage value: 25.9 g/10 min Grade Count:36
Spiral Flow 66.0 - 664 cm26.0 - 261 inAverage value: 129 cm Grade Count:11
Ash 35.0 - 43.0 %35.0 - 43.0 %Average value: 37.0 % Grade Count:9
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 85.0 - 11085.0 - 110Average value: 97.3 Grade Count:37
Hardness, Rockwell R 111 - 125111 - 125Average value: 121 Grade Count:67
Hardness, Shore D 81.0 - 88.081.0 - 88.0Average value: 84.4 Grade Count:3
Ball Indentation Hardness 130 - 310 MPa18900 - 45000 psiAverage value: 246 MPa Grade Count:48
Tensile Strength, Ultimate 14.5 - 350 MPa2100 - 50800 psiAverage value: 179 MPa Grade Count:436
 45.0 - 280 MPa
@Temperature -40.0 - 150 °C
6530 - 40600 psi
@Temperature -40.0 - 302 °F
Average value: 136 MPa Grade Count:12
Tensile Strength, Yield 84.1 - 230 MPa12200 - 33400 psiAverage value: 185 MPa Grade Count:96
 125 - 145 MPa
@Temperature 90.0 - 120 °C
18100 - 21000 psi
@Temperature 194 - 248 °F
Average value: 135 MPa Grade Count:1
Elongation at Break 1.00 - 11.0 %1.00 - 11.0 %Average value: 3.23 % Grade Count:481
 2.00 - 5.60 %
@Temperature -40.0 - 150 °C
2.00 - 5.60 %
@Temperature -40.0 - 302 °F
Average value: 3.63 % Grade Count:10
Elongation at Yield 2.00 - 7.00 %2.00 - 7.00 %Average value: 3.39 % Grade Count:30
Modulus of Elasticity 1.30 - 21.0 GPa189 - 3050 ksiAverage value: 11.0 GPa Grade Count:323
 3.10 - 14.479 GPa
@Temperature -40.0 - 150 °C
450 - 2100.0 ksi
@Temperature -40.0 - 302 °F
Average value: 7.64 GPa Grade Count:11
Flexural Yield Strength 27.6 - 390 MPa4000 - 56600 psiAverage value: 264 MPa Grade Count:385
 130 - 388.175 MPa
@Temperature -40.0 - 121 °C
18900 - 56300.1 psi
@Temperature -40.0 - 250 °F
Average value: 233 MPa Grade Count:11
Flexural Modulus 4.00 - 50.7 GPa580 - 7360 ksiAverage value: 9.99 GPa Grade Count:429
 4.80 - 14.0 GPa
@Temperature -40.0 - 121 °C
696 - 2030 ksi
@Temperature -40.0 - 250 °F
Average value: 8.24 GPa Grade Count:11
Flexural Strain at Break 3.00 - 6.20 %3.00 - 6.20 %Average value: 4.60 % Grade Count:13
 3.70 - 3.70 %
@Temperature 80.0 - 80.0 °C
3.70 - 3.70 %
@Temperature 176 - 176 °F
Average value: 3.70 % Grade Count:1
Compressive Yield Strength 29.6 - 276 MPa4300 - 40000 psiAverage value: 172 MPa Grade Count:12
Poissons Ratio 0.330 - 0.4000.330 - 0.400Average value: 0.358 Grade Count:34
Shear Strength 26.0 - 90.0 MPa3770 - 13100 psiAverage value: 72.8 MPa Grade Count:9
Izod Impact, Notched 0.140 - 5.07 J/cm0.262 - 9.50 ft-lb/inAverage value: 1.52 J/cm Grade Count:156
 0.980665 - 4.64493 J/cm
@Temperature -40.0 - 149 °C
1.83719 - 8.70186 ft-lb/in
@Temperature -40.0 - 300 °F
Average value: 2.61 J/cm Grade Count:4
Izod Impact, Unnotched 0.122 - 16.0 J/cm0.229 - 30.0 ft-lb/inAverage value: 10.5 J/cm Grade Count:53
Izod Impact, Notched (ISO) 2.50 - 47.0 kJ/m²1.19 - 22.4 ft-lb/in²Average value: 13.9 kJ/m² Grade Count:207
 7.70 - 64.0 kJ/m²
@Temperature -40.0 - -30.0 °C
3.66 - 30.5 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 12.0 kJ/m² Grade Count:65
Izod Impact, Unnotched (ISO) 12.0 - 105 kJ/m²5.71 - 50.0 ft-lb/in²Average value: 66.3 kJ/m² Grade Count:28
 60.0 - 105 kJ/m²
@Temperature -30.0 - -30.0 °C
28.6 - 50.0 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 73.3 kJ/m² Grade Count:14
Charpy Impact Unnotched 3.80 J/cm² - NB18.1 ft-lb/in² - NBAverage value: 8.48 J/cm² Grade Count:258
 3.00 - 11.0 J/cm²
@Temperature -40.0 - -20.0 °C
14.3 - 52.4 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 7.43 J/cm² Grade Count:139
Charpy Impact, Notched 0.300 - 3.99 J/cm²1.43 - 19.0 ft-lb/in²Average value: 1.49 J/cm² Grade Count:330
 0.600 - 3.60 J/cm²
@Temperature -40.0 - -20.0 °C
2.86 - 17.1 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 1.18 J/cm² Grade Count:155
Dart Drop, Total Energy  5.35 - 13.9 J
@Temperature -20.0 - -20.0 °C
3.95 - 10.3 ft-lb
@Temperature -4.00 - -4.00 °F
Average value: 9.63 J Grade Count:1
 5.35 - 13.9 J
@Thickness 3.18 - 3.18 mm
3.95 - 10.3 ft-lb
@Thickness 0.125 - 0.125 in
Average value: 9.63 J Grade Count:1
Puncture Energy 3.20 - 17.8 J2.36 - 13.1 ft-lbAverage value: 6.26 J Grade Count:12
 2.60 - 2.80 J
@Temperature -30.0 - -30.0 °C
1.92 - 2.07 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 2.75 J Grade Count:3
Tensile Creep Modulus, 1 hour 7000 - 10800 MPa1.02e+6 - 1.57e+6 psiAverage value: 7880 MPa Grade Count:13
Tensile Creep Modulus, 1000 hours 4250 - 7960 MPa616000 - 1.15e+6 psiAverage value: 6080 MPa Grade Count:19
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 101000 - 1.00e+18 ohm-cm101000 - 1.00e+18 ohm-cmAverage value: 6.78e+15 ohm-cm Grade Count:217
Surface Resistance 3.00e+7 - 1.00e+15 ohm3.00e+7 - 1.00e+15 ohmAverage value: 9.46e+13 ohm Grade Count:131
Dielectric Constant 3.10 - 14.03.10 - 14.0Average value: 4.53 Grade Count:74
Dielectric Strength 15.0 - 90.0 kV/mm380 - 2290 kV/inAverage value: 32.5 kV/mm Grade Count:158
Dissipation Factor 0.00200 - 0.6500.00200 - 0.650Average value: 0.0702 Grade Count:77
Dielectric Loss Index 0.0150 - 0.1500.0150 - 0.150Average value: 0.0825 Grade Count:4
Arc Resistance 60.0 - 180 sec60.0 - 180 secAverage value: 123 sec Grade Count:20
Comparative Tracking Index 250 - 600 V250 - 600 VAverage value: 521 V Grade Count:148
Hot Wire Ignition, HWI 2.00 - 30.0 sec2.00 - 30.0 secAverage value: 14.2 sec Grade Count:15
High Amp Arc Ignition, HAI 0.000 - 120 arcs0.000 - 120 arcsAverage value: 114 arcs Grade Count:15
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min0.394 - 1.00 in/minAverage value: 17.7 mm/min Grade Count:13
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.00 - 95.0 µm/m-°C1.11 - 52.8 µin/in-°FAverage value: 25.6 µm/m-°C Grade Count:119
 4.00 - 21.0 µm/m-°C
@Temperature 55.0 - 160 °C
2.22 - 11.7 µin/in-°F
@Temperature 131 - 320 °F
Average value: 17.3 µm/m-°C Grade Count:6
 16.0 - 21.0 µm/m-°C
@Temperature 35.0 - 55.0 °C
8.89 - 11.7 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 17.3 µm/m-°C Grade Count:11
 16.0 - 21.0 µm/m-°C
@Thickness 2.00 - 2.00 mm
8.89 - 11.7 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 17.3 µm/m-°C Grade Count:11
CTE, linear, Transverse to Flow 7.00 - 110 µm/m-°C3.89 - 61.1 µin/in-°FAverage value: 76.8 µm/m-°C Grade Count:74
 120 - 150 µm/m-°C
@Temperature 55.0 - 160 °C
66.7 - 83.3 µin/in-°F
@Temperature 131 - 320 °F
Average value: 135 µm/m-°C Grade Count:6
Specific Heat Capacity 1.26 - 1.50 J/g-°C0.300 - 0.359 BTU/lb-°FAverage value: 1.45 J/g-°C Grade Count:14
 2.05 - 2.30 J/g-°C
@Temperature 261 - 295 °C
0.490 - 0.550 BTU/lb-°F
@Temperature 502 - 563 °F
Average value: 2.15 J/g-°C Grade Count:9
Thermal Conductivity 0.310 - 0.519 W/m-K2.15 - 3.60 BTU-in/hr-ft²-°FAverage value: 0.381 W/m-K Grade Count:22
 0.220 - 0.250 W/m-K
@Temperature 261 - 295 °C
1.53 - 1.74 BTU-in/hr-ft²-°F
@Temperature 502 - 563 °F
Average value: 0.239 W/m-K Grade Count:10
Melting Point 220 - 325 °C428 - 617 °FAverage value: 260 °C Grade Count:308
Maximum Service Temperature, Air 65.0 - 304 °C149 - 580 °FAverage value: 170 °C Grade Count:68
Deflection Temperature at 0.46 MPa (66 psi) 205 - 290 °C401 - 554 °FAverage value: 255 °C Grade Count:220
Deflection Temperature at 1.8 MPa (264 psi) 107 - 280 °C225 - 536 °FAverage value: 247 °C Grade Count:402
Deflection Temperature at 8.0 MPa 70.0 - 240 °C158 - 464 °FAverage value: 188 °C Grade Count:29
Vicat Softening Point 200 - 265 °C392 - 509 °FAverage value: 246 °C Grade Count:62
Glass Transition Temp, Tg 5.00 - 80.0 °C41.0 - 176 °FAverage value: 46.0 °C Grade Count:18
UL RTI, Electrical 65.0 - 140 °C149 - 284 °FAverage value: 124 °C Grade Count:19
UL RTI, Mechanical with Impact 65.0 - 130 °C149 - 266 °FAverage value: 112 °C Grade Count:17
UL RTI, Mechanical without Impact 65.0 - 140 °C149 - 284 °FAverage value: 128 °C Grade Count:17
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:260
Flame Spread 0.000 - 80.0 mm/min0.000 - 3.15 in/minAverage value: 23.7 mm/min Grade Count:24
Oxygen Index 21.0 - 36.0 %21.0 - 36.0 %Average value: 24.7 % Grade Count:50
Glow Wire Test 600 - 960 °C1110 - 1760 °FAverage value: 755 °C Grade Count:65
 
Processing PropertiesMetricEnglishComments
Processing Temperature 70.0 - 315 °C158 - 599 °FAverage value: 239 °C Grade Count:38
Nozzle Temperature 254 - 315 °C489 - 599 °FAverage value: 288 °C Grade Count:65
Die Temperature 300 - 320 °C572 - 608 °FAverage value: 311 °C Grade Count:6
Melt Temperature 230 - 320 °C446 - 608 °FAverage value: 287 °C Grade Count:244
Mold Temperature 26.7 - 160 °C80.0 - 320 °FAverage value: 87.3 °C Grade Count:261
Injection Velocity 30.0 - 80.0 mm/sec1.18 - 3.15 in/secAverage value: 62.9 mm/sec Grade Count:5
Drying Temperature 65.6 - 130 °C150 - 266 °FAverage value: 82.0 °C Grade Count:212
Moisture Content 0.0200 - 0.200 %0.0200 - 0.200 %Average value: 0.168 % Grade Count:148
Dew Point -28.9 - -17.8 °C-20.0 - 0.000 °FAverage value: -18.5 °C Grade Count:16
Injection Pressure 3.45 - 150 MPa500 - 21800 psiAverage value: 78.9 MPa Grade Count:66
Cushion 0.635 - 0.650 cm0.250 - 0.256 inAverage value: 0.639 cm Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Overview of materials for Nylon 66, 10% Glass Fiber Filled

O2514 / 78013

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.