MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gharda Chemicals G-PAEK™ 1200G Ultra High Performance PEK Polymer
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Unreinforced

Material Notes: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in color

Application Areas: Suitable for high temperature application, high wear & abrasion resistance, high chemical resistance & for metal to plastics conversion, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/cc
Water Absorption 0.080 %
@Time 86400 sec
0.080 %
@Time 24.0 hour
Viscosity 200 cP
@Shear Rate 1000 1/s
200 cP
@Shear Rate 1000 1/s
CR Viscosity at 6 Min; Capillary Rheometer
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/in410°C nozzle, 220°C mold
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/in410°C nozzle, 220°C mold
Crystallinity 40 %40 %DSC
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 103103ASTM D785
Hardness, Shore D 8686
Tensile Strength, Yield  25.0 MPa
@Temperature 250 °C
3630 psi
@Temperature 482 °F
ASTM D638
 35.0 MPa
@Temperature 200 °C
5080 psi
@Temperature 392 °F
ASTM D638
 55.0 MPa
@Temperature 150 °C
7980 psi
@Temperature 302 °F
ASTM D638
 75.0 MPa
@Temperature 100 °C
10900 psi
@Temperature 212 °F
ASTM D638
 100 - 110 MPa
@Temperature 23.0 °C
14500 - 16000 psi
@Temperature 73.4 °F
ASTM D638
 140 MPa
@Temperature -10.0 °C
20300 psi
@Temperature 14.0 °F
ASTM D638
 160 MPa
@Temperature -50.0 °C
23200 psi
@Temperature -58.0 °F
ASTM D638
Elongation at Break 10 - 15 %10 - 15 %ASTM D638
Tensile Modulus 4.20 GPa609 ksiASTM D638
Flexural Strength 185 - 190 MPa26800 - 27600 psiASTM D790
Flexural Modulus 4.10 GPa595 ksiASTM D790
Izod Impact, Notched 0.550 - 0.600 J/cm1.03 - 1.12 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistivity per Square 1.00e+16 ohm1.00e+16 ohmASTM D257
Dielectric Strength 16.0 kV/mm
@Thickness 3.20 mm
406 kV/in
@Thickness 0.126 in
ASTM D149
Arc Resistance 175 sec175 secat 500 Volts; ASTM D495
Comparative Tracking Index 145 V145 Vper 50 drops; ASTM D3638
 
Thermal PropertiesMetricEnglishComments
Melting Point 370 - 372 °C698 - 702 °FDSC
Deflection Temperature at 1.8 MPa (264 psi) 167 °C333 °F
Glass Transition Temp, Tg 152 - 154 °C306 - 309 °FDSC/onset
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 385 - 410 °C725 - 770 °F
Nozzle Temperature 410 °C770 °F
Mold Temperature 200 - 220 °C392 - 428 °F
Drying Temperature 150 °C302 °F
Dry Time 4 - 6 hour4 - 6 hour
 
Descriptive Properties
Hopper/ Throat Temperature60-80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade
Gharda Chemicals G-PAEK™ 1200P Ultra High Performance PEK Polymer
Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced
Gharda Chemicals G-PAEK™ 1230CF Ultra High Performance PEK Polymer

PGHARD991 / 108526

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.