MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Gharda Chemicals G-PAEK™ 1230CF Ultra High Performance PEK Polymer
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Carbon Fiber Filled

Material Notes: Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in color

Application Areas: Suitable for high temperature application, where higher strength & stiffness needed in load bearing application. Excellent wear resistance. Chemically resistant to aggressive environments, suitable for sterilization for medical and food contact applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/cc
Water Absorption 0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
Linear Mold Shrinkage, Flow 0.0011 cm/cm0.0011 in/in410°C nozzle, 220°C mold
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in410°C nozzle, 220°C mold
Crystallinity 40 %40 %DSC
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 108108ASTM D785
Hardness, Shore D 9191
Tensile Strength, Yield  75.0 MPa
@Temperature 250 °C
10900 psi
@Temperature 482 °F
ASTM D638
 95.0 MPa
@Temperature 200 °C
13800 psi
@Temperature 392 °F
ASTM D638
 125 MPa
@Temperature 150 °C
18100 psi
@Temperature 302 °F
ASTM D638
 185 MPa
@Temperature 100 °C
26800 psi
@Temperature 212 °F
ASTM D638
 250 MPa
@Temperature 23.0 °C
36300 psi
@Temperature 73.4 °F
ASTM D638
 260 MPa
@Temperature -10.0 °C
37700 psi
@Temperature 14.0 °F
ASTM D638
 275 MPa
@Temperature -50.0 °C
39900 psi
@Temperature -58.0 °F
ASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Tensile Modulus 22.6 GPa3280 ksiASTM D638
Flexural Strength 360 MPa52200 psiASTM D790
Flexural Modulus 22.0 GPa3190 ksiASTM D790
Izod Impact, Notched 0.500 J/cm0.937 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 370 - 372 °C698 - 702 °FDSC
Deflection Temperature at 1.8 MPa (264 psi) 368 °C694 °F
Glass Transition Temp, Tg 152 - 154 °C306 - 309 °FDSC/onset
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 390 - 425 °C734 - 797 °F
Nozzle Temperature 425 °C797 °F
Mold Temperature 200 - 220 °C392 - 428 °F
Drying Temperature 150 °C302 °F
Dry Time 4 - 6 hour4 - 6 hour
 
Descriptive Properties
Hopper/ Throat Temperature60-80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gharda Chemicals G-PAEK™ 1230FC Ultra High Performance PEK Polymer
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer
EMS-Grivory Grivory® HT1V-3 FWA black 9225 PA6T/6I-GF30
Ensinger TECASINT 1011 Polyimide (PI)
Gharda Chemicals G-PAEK™ 1200G Ultra High Performance PEK Polymer

PGHARD993 / 108528

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.