MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Gharda Chemicals G-PAEK™ 1200G Ultra High Performance PEK Polymer
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Unreinforced

Material Notes: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in color

Application Areas: Suitable for high temperature application, high wear & abrasion resistance, high chemical resistance & for metal to plastics conversion, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/cc
Water Absorption 0.080 %
@Time 86400 sec
Viscosity 200 cP
@Shear Rate 1000 1/s
CR Viscosity at 6 Min; Capillary Rheometer
Linear Mold Shrinkage, Flow 0.010 cm/cm410°C nozzle, 220°C mold
Linear Mold Shrinkage, Transverse 0.013 cm/cm410°C nozzle, 220°C mold
Crystallinity 40 %DSC
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 103ASTM D785
Hardness, Shore D 86
Tensile Strength, Yield 25.0 MPa
@Temperature 250 °C
ASTM D638
 35.0 MPa
@Temperature 200 °C
ASTM D638
 55.0 MPa
@Temperature 150 °C
ASTM D638
 75.0 MPa
@Temperature 100 °C
ASTM D638
 100 - 110 MPa
@Temperature 23.0 °C
ASTM D638
 140 MPa
@Temperature -10.0 °C
ASTM D638
 160 MPa
@Temperature -50.0 °C
ASTM D638
Elongation at Break 10 - 15 %ASTM D638
Tensile Modulus 4.20 GPaASTM D638
Flexural Strength 185 - 190 MPaASTM D790
Flexural Modulus 4.10 GPaASTM D790
Izod Impact, Notched 55.0 - 60.0 J/mASTM D256
Izod Impact, Unnotched NBASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Surface Resistivity per Square 1.00e+16 ohmASTM D257
Dielectric Strength 16.0 kV/mm
@Thickness 3.20 mm
ASTM D149
Arc Resistance 175 secat 500 Volts; ASTM D495
Comparative Tracking Index 145 Vper 50 drops; ASTM D3638
 
Thermal PropertiesOriginal ValueComments
Melting Point 370 - 372 °CDSC
Deflection Temperature at 1.8 MPa (264 psi) 167 °C
Glass Transition Temp, Tg 152 - 154 °CDSC/onset
Flammability, UL94 V-0
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 385 - 410 °C
Nozzle Temperature 410 °C
Mold Temperature 200 - 220 °C
Drying Temperature 150 °C
Dry Time 4 - 6 hour
 
Descriptive Properties
Hopper/ Throat Temperature60-80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade
Gharda Chemicals G-PAEK™ 1200P Ultra High Performance PEK Polymer
Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced
Gharda Chemicals G-PAEK™ 1230CF Ultra High Performance PEK Polymer

PGHARD991 / 108526

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.