MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetherketoneetherketoneketone (PEKEKK), Wear Resistant

Material Notes: TECAPEEK® ST is a multipurpose semi-crystalline material from the polyaryletherketone family based on PEKEKK that features improved mechanical properties at higher temperatures. The benefits of TECAPEEK® ST compared to standard TECAPEEK® are that of a higher heat distortion temperature (HDT), better strength and stiffness of machined components and a higher flexural strength combined with a higher glass transition point.
  • Excellent mechanical properties at higher temperatures
  • High heat distortion temperature
  • Excellent chemical resistance
  • Low moisture absorption
  • Electrically insulating
  • Easy to machine (unfilled)
  • Good dimensional stability
  • High purity

Target industries for TECAPEEK® ST are Oil and Gas, Semiconductor, Chemical and Automotive, crude petroleum extraction and drilling. Possible applications include turbocharger impellers, seal rings and other down hole parts, gears, and test sockets.

Information Provided by Ensinger Inc.

Key Words: PEKEKK
Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccD792
Density 1.30 g/cc0.0470 lb/in³D792
Moisture Absorption at Equilibrium 0.050 %0.050 %RH 50%; D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 130 MPa18900 psiD638
Elongation at Yield 11 %11 %ISO527
Tensile Modulus 4.40 GPa638 ksi1mm/min; D638
Charpy Impact 5.80 J
@Temperature 22.8 °C
4.28 ft-lb
@Temperature 73.0 °F
ISO179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC60093
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmIEC60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 49.0 µm/m-°C27.2 µin/in-°FE831
Melting Point 387 °C729 °FD3418
Maximum Service Temperature, Air 260 °C500 °F
Deflection Temperature at 1.8 MPa (264 psi) 172 °C342 °FD648
Glass Transition Temp, Tg 162 °C324 °FD3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
VICTREX ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Overview of materials for Polyetheretherketone, Unreinforced
Gharda Chemicals G-PAEK™ 1200G Ultra High Performance PEK Polymer
RTP Company RTP 3999X56542A Polyetherketoneetherketoneketone (PEKEKK), Wear Resistant

PENSIN996 / 139292

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.